General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 8 g/cm³ Show Material materials with Densidad of 8 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Austenitic Stainless Steel |
Elongación | 20.0 °C | 35 % Show Material materials with Elongación of 35 % | |
Elongación transversal | 20.0 °C | 30 % Show Material materials with Elongación transversal of 30 % | |
Límite elástico Rp 0,2 | 20.0 °C | 205 MPa Show Material materials with Límite elástico Rp 0,2 of 205 MPa | |
50.0 °C | 184 MPa Show Material materials with Límite elástico Rp 0,2 of 184 MPa | ||
100.0 °C | 177 MPa Show Material materials with Límite elástico Rp 0,2 of 177 MPa | ||
150.0 °C | 162 MPa Show Material materials with Límite elástico Rp 0,2 of 162 MPa | ||
200.0 °C | 147 MPa Show Material materials with Límite elástico Rp 0,2 of 147 MPa | ||
250.0 °C | 137 MPa Show Material materials with Límite elástico Rp 0,2 of 137 MPa | ||
300.0 °C | 127 MPa Show Material materials with Límite elástico Rp 0,2 of 127 MPa | ||
350.0 °C | 122 MPa Show Material materials with Límite elástico Rp 0,2 of 122 MPa | ||
400.0 °C | 118 MPa Show Material materials with Límite elástico Rp 0,2 of 118 MPa | ||
450.0 °C | 113 MPa Show Material materials with Límite elástico Rp 0,2 of 113 MPa | ||
500.0 °C | 108 MPa Show Material materials with Límite elástico Rp 0,2 of 108 MPa | ||
550.0 °C | 103 MPa Show Material materials with Límite elástico Rp 0,2 of 103 MPa | ||
Límite elástico Rp 1,0 | 20.0 °C | 245 MPa Show Material materials with Límite elástico Rp 1,0 of 245 MPa | |
50.0 °C | 228 MPa Show Material materials with Límite elástico Rp 1,0 of 228 MPa | ||
100.0 °C | 211 MPa Show Material materials with Límite elástico Rp 1,0 of 211 MPa | ||
150.0 °C | 194 MPa Show Material materials with Límite elástico Rp 1,0 of 194 MPa | ||
200.0 °C | 177 MPa Show Material materials with Límite elástico Rp 1,0 of 177 MPa | ||
250.0 °C | 167 MPa Show Material materials with Límite elástico Rp 1,0 of 167 MPa | ||
300.0 °C | 157 MPa Show Material materials with Límite elástico Rp 1,0 of 157 MPa | ||
350.0 °C | 152 MPa Show Material materials with Límite elástico Rp 1,0 of 152 MPa | ||
400.0 °C | 147 MPa Show Material materials with Límite elástico Rp 1,0 of 147 MPa | ||
450.0 °C | 142 MPa Show Material materials with Límite elástico Rp 1,0 of 142 MPa | ||
500.0 °C | 137 MPa Show Material materials with Límite elástico Rp 1,0 of 137 MPa | ||
550.0 °C | 132 MPa Show Material materials with Límite elástico Rp 1,0 of 132 MPa | ||
Límite elástico transversal Rp 0,2 | 20.0 °C | 205 MPa Show Material materials with Límite elástico transversal Rp 0,2 of 205 MPa | |
Límite elástico transversal Rp 1,0 | 20.0 °C | 245 MPa Show Material materials with Límite elástico transversal Rp 1,0 of 245 MPa | |
Módulo de cizallamiento | 23.0 °C | 77 GPa Show Material materials with Módulo de cizallamiento of 77 GPa | Typical for Austenitic Stainless Steel |
Módulo elástico | 20.0 °C | 200 GPa Show Material materials with Módulo elástico of 200 GPa | |
100.0 °C | 194 GPa Show Material materials with Módulo elástico of 194 GPa | ||
200.0 °C | 186 GPa Show Material materials with Módulo elástico of 186 GPa | ||
300.0 °C | 179 GPa Show Material materials with Módulo elástico of 179 GPa | ||
400.0 °C | 172 GPa Show Material materials with Módulo elástico of 172 GPa | ||
500.0 °C | 165 GPa Show Material materials with Módulo elástico of 165 GPa | ||
600.0 °C | 155 GPa Show Material materials with Módulo elástico of 155 GPa | ||
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 20.0 °C | 500 J/(kg·K) Show Material materials with Calor específico of 500 J/(kg·K) | |
Coeficiente de dilatación térmica | 100.0 °C | 1.6E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.6E-5 1/K | |
200.0 °C | 1.65E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.65E-5 1/K | ||
300.0 °C | 1.7E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.7E-5 1/K | ||
400.0 °C | 1.75E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.75E-5 1/K | ||
500.0 °C | 1.8E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.8E-5 1/K | ||
600.0 °C | 1.85E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.85E-5 1/K | ||
Conductividad térmica | 20.0 °C | 15 W/(m·K) Show Material materials with Conductividad térmica of 15 W/(m·K) | |
Temperatura de fusión | 1230 - 1480 °C Show Material materials with Temperatura de fusión of 1230 - 1480 °C | Typical for Austenitic Stainless Steel |
Eléctrico
Property | Temperature | Value |
---|---|---|
Resistividad eléctrica | 20.0 °C | 7.5E-7 Ω·m Show Material materials with Resistividad eléctrica of 7.5E-7 Ω·m |
Chemical properties
Property | Value |
---|---|
Azufre | 0.015 % Show Material materials with Azufre of 0.015 % |
Carbono | 0.04 - 0.08 % Show Material materials with Carbono of 0.04 - 0.08 % |
Cromo | 16 - 18 % Show Material materials with Cromo of 16 - 18 % |
Fósforo | 0.04 % Show Material materials with Fósforo of 0.04 % |
Manganeso | 2 % Show Material materials with Manganeso of 2 % |
Molibdeno | 2 - 2.5 % Show Material materials with Molibdeno of 2 - 2.5 % |
Nitrógeno | 0.11 % Show Material materials with Nitrógeno of 0.11 % |
Níquel | 12 - 14 % Show Material materials with Níquel of 12 - 14 % |
Silicona | 0.75 % Show Material materials with Silicona of 0.75 % |