Wrought Copper Brass Yellow Brass
EN 1652 Grade CuZn40 R340Titanio puro
DIN 17850 Grade Ti1Pd AnnealedAcero inoxidable austenítico
DIN 17440 Grade X6CrNiTi18-10 solution heat-treated and quenchedAcero inoxidable austenítico
DIN 17440 Grade X6CrNiMoTi17-12-2 solution heat-treated and quenchedAcero inoxidable austenítico
EN 10272 Grade X1NiCrMoCu31-27-4 solution annealed (+AT)Acero inoxidable austenítico
EN 10028-7 Grade X6CrNi18-10 solution annealed (+AT)Acero inoxidable austenítico
EN 10272 Grade X2CrNi18-9 solution annealed (+AT)Leaded Brass
EN 1652 Grade CuZn39Pb0.5 R340Aleación casi alfa
VdTÜV WB 230-3 Grade TiNi0.8Mo0.3 AnnealedSuministrada por:
2 proveedores de Matmatch
Acero inoxidable austenítico
EN 10216-5 Grade X6CrNiTi18-10 solution annealed (+AT)Acero inoxidable austenítico
EN 10216-5 Grade X6CrNiMoTi17-12-2 solution annealed (+AT)Acero inoxidable austenítico
EN 10216-5 Grade X6CrNiMo17-13 solution annealed (+AT)Acero inoxidable austenítico
EN 10028-7 Grade X6CrNi23-13 solution annealed (+AT)Acero inoxidable austenítico
EN 10028-7 Grade X6CrNi25-20 solution annealed (+AT)Acero inoxidable austenítico
EN 10216-5 Grade X6CrNi18-10 solution annealed (+AT)Acero inoxidable austenítico
EN 10217-7 Grade X6CrNiMoTi17-12-2 solution annealed (+AT)Acero inoxidable austenítico
EN 10217-7 Grade X6CrNiTi18-10 solution annealed (+AT)Leaded Brass
EN 12166 Grade CuZn40Pb2 H075