General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 7.83 g/cm³ Show Material materials with Densidad of 7.83 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.29 [-] Show Material materials with Coeficiente de Poisson of 0.29 [-] | Typical for Low Carbon Steel |
Elongación | 20.0 °C | 21 - 23 % Show Material materials with Elongación of 21 - 23 % | |
Límite elástico | 20.0 °C | 330 - 355 MPa Show Material materials with Límite elástico of 330 - 355 MPa | |
200.0 °C | 255 MPa Show Material materials with Límite elástico of 255 MPa | ||
250.0 °C | 235 MPa Show Material materials with Límite elástico of 235 MPa | ||
300.0 °C | 216 MPa Show Material materials with Límite elástico of 216 MPa | ||
350.0 °C | 196 MPa Show Material materials with Límite elástico of 196 MPa | ||
400.0 °C | 167 MPa Show Material materials with Límite elástico of 167 MPa | ||
Límite elástico Rp 0,2 | 20.0 °C | 320 - 345 MPa Show Material materials with Límite elástico Rp 0,2 of 320 - 345 MPa | |
50.0 °C | 319 - 343 MPa Show Material materials with Límite elástico Rp 0,2 of 319 - 343 MPa | ||
100.0 °C | 294 - 323 MPa Show Material materials with Límite elástico Rp 0,2 of 294 - 323 MPa | ||
150.0 °C | 275 - 299 MPa Show Material materials with Límite elástico Rp 0,2 of 275 - 299 MPa | ||
200.0 °C | 255 - 275 MPa Show Material materials with Límite elástico Rp 0,2 of 255 - 275 MPa | ||
250.0 °C | 234 - 252 MPa Show Material materials with Límite elástico Rp 0,2 of 234 - 252 MPa | ||
300.0 °C | 215 - 232 MPa Show Material materials with Límite elástico Rp 0,2 of 215 - 232 MPa | ||
350.0 °C | 196 - 214 MPa Show Material materials with Límite elástico Rp 0,2 of 196 - 214 MPa | ||
400.0 °C | 167 - 202 MPa Show Material materials with Límite elástico Rp 0,2 of 167 - 202 MPa | ||
Módulo de cizallamiento | 23.0 °C | 82 GPa Show Material materials with Módulo de cizallamiento of 82 GPa | Typical for Low Carbon Steel |
Módulo elástico | -100.0 °C | 217 GPa Show Material materials with Módulo elástico of 217 GPa | |
20.0 °C | 212 GPa Show Material materials with Módulo elástico of 212 GPa | ||
100.0 °C | 207 GPa Show Material materials with Módulo elástico of 207 GPa | ||
200.0 °C | 199 GPa Show Material materials with Módulo elástico of 199 GPa | ||
300.0 °C | 192 GPa Show Material materials with Módulo elástico of 192 GPa | ||
400.0 °C | 184 GPa Show Material materials with Módulo elástico of 184 GPa | ||
500.0 °C | 175 GPa Show Material materials with Módulo elástico of 175 GPa | ||
600.0 °C | 164 GPa Show Material materials with Módulo elástico of 164 GPa | ||
Resistencia a la tracción | 20.0 °C | 490 - 630 MPa Show Material materials with Resistencia a la tracción of 490 - 630 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | -100.0 °C | 423 J/(kg·K) Show Material materials with Calor específico of 423 J/(kg·K) | |
20.0 °C | 461 J/(kg·K) Show Material materials with Calor específico of 461 J/(kg·K) | ||
100.0 °C | 479 J/(kg·K) Show Material materials with Calor específico of 479 J/(kg·K) | ||
200.0 °C | 499 J/(kg·K) Show Material materials with Calor específico of 499 J/(kg·K) | ||
300.0 °C | 517 J/(kg·K) Show Material materials with Calor específico of 517 J/(kg·K) | ||
400.0 °C | 536 J/(kg·K) Show Material materials with Calor específico of 536 J/(kg·K) | ||
500.0 °C | 558 J/(kg·K) Show Material materials with Calor específico of 558 J/(kg·K) | ||
600.0 °C | 587 J/(kg·K) Show Material materials with Calor específico of 587 J/(kg·K) | ||
Coeficiente de dilatación térmica | -100.0 °C | 1.08E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.08E-5 1/K | |
20.0 °C | 1.19E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.19E-5 1/K | ||
100.0 °C | 1.25E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.25E-5 1/K | ||
200.0 °C | 1.3E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.3E-5 1/K | ||
300.0 °C | 1.36E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.36E-5 1/K | ||
400.0 °C | 1.41E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.41E-5 1/K | ||
500.0 °C | 1.45E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.45E-5 1/K | ||
600.0 °C | 1.49E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.49E-5 1/K | ||
Conductividad térmica | -100.0 °C | 37.6 W/(m·K) Show Material materials with Conductividad térmica of 37.6 W/(m·K) | |
20.0 °C | 42.2 W/(m·K) Show Material materials with Conductividad térmica of 42.2 W/(m·K) | ||
100.0 °C | 43.2 W/(m·K) Show Material materials with Conductividad térmica of 43.2 W/(m·K) | ||
200.0 °C | 42.9 W/(m·K) Show Material materials with Conductividad térmica of 42.9 W/(m·K) | ||
300.0 °C | 41.2 W/(m·K) Show Material materials with Conductividad térmica of 41.2 W/(m·K) | ||
400.0 °C | 39.1 W/(m·K) Show Material materials with Conductividad térmica of 39.1 W/(m·K) | ||
500.0 °C | 36.6 W/(m·K) Show Material materials with Conductividad térmica of 36.6 W/(m·K) | ||
600.0 °C | 34.1 W/(m·K) Show Material materials with Conductividad térmica of 34.1 W/(m·K) | ||
Difusividad térmica | -100.0 °C | 12.9 mm²/s Show Material materials with Difusividad térmica of 12.9 mm²/s | |
20.0 °C | 11.7 mm²/s Show Material materials with Difusividad térmica of 11.7 mm²/s | ||
100.0 °C | 11.2 mm²/s Show Material materials with Difusividad térmica of 11.2 mm²/s | ||
200.0 °C | 10.3 mm²/s Show Material materials with Difusividad térmica of 10.3 mm²/s | ||
300.0 °C | 9.4 mm²/s Show Material materials with Difusividad térmica of 9.4 mm²/s | ||
400.0 °C | 8.3 mm²/s Show Material materials with Difusividad térmica of 8.3 mm²/s | ||
500.0 °C | 7.1 mm²/s Show Material materials with Difusividad térmica of 7.1 mm²/s | ||
600.0 °C | 5.7 mm²/s Show Material materials with Difusividad térmica of 5.7 mm²/s | ||
Temperatura de fusión | 1480 - 1526 °C Show Material materials with Temperatura de fusión of 1480 - 1526 °C | Typical for Low Carbon Steel | |
Temperatura máx. de funcionamiento | 500 °C Show Material materials with Temperatura máx. de funcionamiento of 500 °C | Typical for Carbon Steel |
Eléctrico
Property | Temperature | Value |
---|---|---|
Resistividad eléctrica | -100.0 °C | 1.82E-7 Ω·m Show Material materials with Resistividad eléctrica of 1.82E-7 Ω·m |
20.0 °C | 2.47E-7 Ω·m Show Material materials with Resistividad eléctrica of 2.47E-7 Ω·m | |
100.0 °C | 2.96E-7 Ω·m Show Material materials with Resistividad eléctrica of 2.96E-7 Ω·m | |
200.0 °C | 3.68E-7 Ω·m Show Material materials with Resistividad eléctrica of 3.68E-7 Ω·m | |
300.0 °C | 4.55E-7 Ω·m Show Material materials with Resistividad eléctrica of 4.55E-7 Ω·m | |
400.0 °C | 5.56E-7 Ω·m Show Material materials with Resistividad eléctrica of 5.56E-7 Ω·m | |
500.0 °C | 6.75E-7 Ω·m Show Material materials with Resistividad eléctrica of 6.75E-7 Ω·m | |
600.0 °C | 8.13E-7 Ω·m Show Material materials with Resistividad eléctrica of 8.13E-7 Ω·m | |
Magnético
Property | Value | Comment |
---|---|---|
Temperatura de Curie | 770 °C Show Material materials with Temperatura de Curie of 770 °C | Typical for Low Carbon Steel |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.02 - 0.06 % Show Material materials with Aluminio of 0.02 - 0.06 % |
Azufre | 0.01 - 0.015 % Show Material materials with Azufre of 0.01 - 0.015 % |
Carbono | 0.18 - 0.2 % Show Material materials with Carbono of 0.18 - 0.2 % |
Cobre | 0.2 - 0.3 % Show Material materials with Cobre of 0.2 - 0.3 % |
Cromo | 0.3 % Show Material materials with Cromo of 0.3 % |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % |
Manganeso | 0.9 - 1.7 % Show Material materials with Manganeso of 0.9 - 1.7 % |
Molibdeno | 0.08 % Show Material materials with Molibdeno of 0.08 % |
Niobio | 0.05 % Show Material materials with Niobio of 0.05 % |
Nitrógeno | 0.02 % Show Material materials with Nitrógeno of 0.02 % |
Níquel | 0.3 - 0.5 % Show Material materials with Níquel of 0.3 - 0.5 % |
Silicona | 0.1 - 0.5 % Show Material materials with Silicona of 0.1 - 0.5 % |
Vanadio | 0.1 % Show Material materials with Vanadio of 0.1 % |