Resistividad eléctrica: 2.47E-7 Ω·m

Quick Comparison

Acero bajo en carbono

EN 10025-2 Grade S355J2 normalized or normalized formed (+N)

Suministrada por:

2 proveedores de Matmatch

Acero bajo en carbono

EN 10025-2 Grade S355K2 normalized or normalized formed (+N)

Suministrada por:

2 proveedores de Matmatch

Acero bajo en carbono

EN 10028-3 Grade P355NH normalized or normalized formed (+N)

Suministrada por:

2 proveedores de Matmatch

Acero bajo en carbono

EN 10028-3 Grade P355NL1 normalized or normalized formed (+N)

Suministrada por:

2 proveedores de Matmatch

Acero bajo en carbono

EN 10028-3 Grade P355NL2 normalized or normalized formed (+N)

Suministrada por:

2 proveedores de Matmatch

Acero bajo en carbono

EN 10025-3 Grade S355N normalized or normalized formed (+N)

Suministrada por:

2 proveedores de Matmatch

Acero bajo en carbono

EN 10025-3 Grade S355NL normalized or normalized formed (+N)

Suministrada por:

2 proveedores de Matmatch

Acero bajo en carbono

EN 10025-2 Grade S355JR normalized or normalized formed (+N)

Suministrada por:

1 proveedor Matmatch

Medium Carbon Steel

EN 10028-3 Grade P355N normalized or normalized formed (+N)

Suministrada por:

2 proveedores de Matmatch

Acero bajo en carbono

EN 10149-3 Grade S420NC normalized or normalized formed (+N)

Suministrada por:

1 proveedor Matmatch

Medium Carbon Steel

ISO 683-1 Grade C45 quenched and tempered (+QT)

Suministrada por:

1 proveedor Matmatch

Medium Carbon Steel

ISO 683-1 Grade C45 quenched and tempered (+QT)

Suministrada por:

1 proveedor Matmatch

Nickel Molybdenum Steel

EN 10028-2 Grade 20MnMoNi4-5 quenched and tempered (+QT)

Suministrada por:

1 proveedor Matmatch

Medium Carbon Steel

ISO 683-1 Grade C45E quenched and tempered (+QT)

Suministrada por:

1 proveedor Matmatch

Wrought Copper High Copper Alloy

ASTM B196 Grade C17200 TB00

Wrought Copper High Copper Alloy

ASTM B194 Grade C17200 TD04

Wrought Copper High Copper Alloy

ASTM B768 Grade C17510 TH04

Wrought Copper High Copper Alloy

EN 1652 Grade C17200 TF00
Página 1 de 13