General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 7.84 - 7.85 g/cm³ Show Material materials with Densidad of 7.84 - 7.85 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Coeficiente de Poisson | 20.0 °C | 0.28 [-] Show Material materials with Coeficiente de Poisson of 0.28 [-] |
100.0 °C | 0.29 [-] Show Material materials with Coeficiente de Poisson of 0.29 [-] | |
200.0 °C | 0.29 [-] Show Material materials with Coeficiente de Poisson of 0.29 [-] | |
300.0 °C | 0.29 [-] Show Material materials with Coeficiente de Poisson of 0.29 [-] | |
400.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | |
500.0 °C | 0.31 [-] Show Material materials with Coeficiente de Poisson of 0.31 [-] | |
600.0 °C | 0.31 [-] Show Material materials with Coeficiente de Poisson of 0.31 [-] | |
Elongación | 20.0 °C | 17 - 18 % Show Material materials with Elongación of 17 - 18 % |
Límite elástico | 20.0 °C | 250 - 310 MPa Show Material materials with Límite elástico of 250 - 310 MPa |
Límite elástico Rp 0,2 | 50.0 °C | 250 - 288 MPa Show Material materials with Límite elástico Rp 0,2 of 250 - 288 MPa |
100.0 °C | 237 - 266 MPa Show Material materials with Límite elástico Rp 0,2 of 237 - 266 MPa | |
150.0 °C | 228 - 254 MPa Show Material materials with Límite elástico Rp 0,2 of 228 - 254 MPa | |
200.0 °C | 222 - 248 MPa Show Material materials with Límite elástico Rp 0,2 of 222 - 248 MPa | |
250.0 °C | 219 - 243 MPa Show Material materials with Límite elástico Rp 0,2 of 219 - 243 MPa | |
300.0 °C | 213 - 236 MPa Show Material materials with Límite elástico Rp 0,2 of 213 - 236 MPa | |
350.0 °C | 204 - 225 MPa Show Material materials with Límite elástico Rp 0,2 of 204 - 225 MPa | |
400.0 °C | 191 - 212 MPa Show Material materials with Límite elástico Rp 0,2 of 191 - 212 MPa | |
450.0 °C | 178 - 197 MPa Show Material materials with Límite elástico Rp 0,2 of 178 - 197 MPa | |
500.0 °C | 167 - 185 MPa Show Material materials with Límite elástico Rp 0,2 of 167 - 185 MPa | |
Módulo de cizallamiento | 20.0 °C | 82.81 GPa Show Material materials with Módulo de cizallamiento of 82.81 GPa |
100.0 °C | 80.65 GPa Show Material materials with Módulo de cizallamiento of 80.65 GPa | |
200.0 °C | 77.87 GPa Show Material materials with Módulo de cizallamiento of 77.87 GPa | |
300.0 °C | 74.93 GPa Show Material materials with Módulo de cizallamiento of 74.93 GPa | |
400.0 °C | 71.22 GPa Show Material materials with Módulo de cizallamiento of 71.22 GPa | |
500.0 °C | 66.9 GPa Show Material materials with Módulo de cizallamiento of 66.9 GPa | |
600.0 °C | 62.11 GPa Show Material materials with Módulo de cizallamiento of 62.11 GPa | |
Módulo elástico | -100.0 °C | 217 GPa Show Material materials with Módulo elástico of 217 GPa |
20.0 °C | 212 - 212.43 GPa Show Material materials with Módulo elástico of 212 - 212.43 GPa | |
100.0 °C | 207 - 207.49 GPa Show Material materials with Módulo elástico of 207 - 207.49 GPa | |
200.0 °C | 199 - 201.15 GPa Show Material materials with Módulo elástico of 199 - 201.15 GPa | |
300.0 °C | 192 - 193.89 GPa Show Material materials with Módulo elástico of 192 - 193.89 GPa | |
400.0 °C | 184 - 185.24 GPa Show Material materials with Módulo elástico of 184 - 185.24 GPa | |
500.0 °C | 174.89 - 175 GPa Show Material materials with Módulo elástico of 174.89 - 175 GPa | |
600.0 °C | 163.15 - 164 GPa Show Material materials with Módulo elástico of 163.15 - 164 GPa | |
Resistencia a la tracción | 20.0 °C | 460 - 630 MPa Show Material materials with Resistencia a la tracción of 460 - 630 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | -100.0 °C | 423 J/(kg·K) Show Material materials with Calor específico of 423 J/(kg·K) | |
20.0 °C | 461 J/(kg·K) Show Material materials with Calor específico of 461 J/(kg·K) | ||
100.0 °C | 479 J/(kg·K) Show Material materials with Calor específico of 479 J/(kg·K) | ||
200.0 °C | 499 J/(kg·K) Show Material materials with Calor específico of 499 J/(kg·K) | ||
300.0 °C | 517 J/(kg·K) Show Material materials with Calor específico of 517 J/(kg·K) | ||
400.0 °C | 536 J/(kg·K) Show Material materials with Calor específico of 536 J/(kg·K) | ||
500.0 °C | 558 J/(kg·K) Show Material materials with Calor específico of 558 J/(kg·K) | ||
600.0 °C | 587 J/(kg·K) Show Material materials with Calor específico of 587 J/(kg·K) | ||
Coeficiente de dilatación térmica | -100.0 °C | 1.05E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.05E-5 1/K | |
20.0 °C | 1.15E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.15E-5 1/K | ||
100.0 °C | 1.21E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.21E-5 1/K | ||
200.0 °C | 1.27E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.27E-5 1/K | ||
300.0 °C | 1.32E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.32E-5 1/K | ||
400.0 °C | 1.36E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.36E-5 1/K | ||
500.0 °C | 1.4E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.4E-5 1/K | ||
600.0 °C | 1.44E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.44E-5 1/K | ||
Conductividad térmica | 20.0 °C | 34.9 W/(m·K) Show Material materials with Conductividad térmica of 34.9 W/(m·K) | |
100.0 °C | 37.3 W/(m·K) Show Material materials with Conductividad térmica of 37.3 W/(m·K) | ||
200.0 °C | 38.2 W/(m·K) Show Material materials with Conductividad térmica of 38.2 W/(m·K) | ||
300.0 °C | 37.8 W/(m·K) Show Material materials with Conductividad térmica of 37.8 W/(m·K) | ||
400.0 °C | 36.6 W/(m·K) Show Material materials with Conductividad térmica of 36.6 W/(m·K) | ||
500.0 °C | 35.2 W/(m·K) Show Material materials with Conductividad térmica of 35.2 W/(m·K) | ||
600.0 °C | 33.6 W/(m·K) Show Material materials with Conductividad térmica of 33.6 W/(m·K) | ||
Difusividad térmica | 20.0 °C | 9.7 mm²/s Show Material materials with Difusividad térmica of 9.7 mm²/s | |
100.0 °C | 9.6 mm²/s Show Material materials with Difusividad térmica of 9.6 mm²/s | ||
200.0 °C | 9.2 mm²/s Show Material materials with Difusividad térmica of 9.2 mm²/s | ||
300.0 °C | 8.5 mm²/s Show Material materials with Difusividad térmica of 8.5 mm²/s | ||
400.0 °C | 7.8 mm²/s Show Material materials with Difusividad térmica of 7.8 mm²/s | ||
500.0 °C | 6.8 mm²/s Show Material materials with Difusividad térmica of 6.8 mm²/s | ||
600.0 °C | 5.7 mm²/s Show Material materials with Difusividad térmica of 5.7 mm²/s | ||
Temperatura de fusión | 1382 - 1529 °C Show Material materials with Temperatura de fusión of 1382 - 1529 °C | Typical for Chromium Molybdenum Steel | |
Temperatura máx. de funcionamiento, largo | 400 - 550 °C Show Material materials with Temperatura máx. de funcionamiento, largo of 400 - 550 °C |
Eléctrico
Property | Temperature | Value |
---|---|---|
Resistividad eléctrica | 20.0 °C | 2.98E-7 Ω·m Show Material materials with Resistividad eléctrica of 2.98E-7 Ω·m |
100.0 °C | 3.43E-7 Ω·m Show Material materials with Resistividad eléctrica of 3.43E-7 Ω·m | |
200.0 °C | 4.13E-7 Ω·m Show Material materials with Resistividad eléctrica of 4.13E-7 Ω·m | |
300.0 °C | 4.97E-7 Ω·m Show Material materials with Resistividad eléctrica of 4.97E-7 Ω·m | |
400.0 °C | 5.95E-7 Ω·m Show Material materials with Resistividad eléctrica of 5.95E-7 Ω·m | |
500.0 °C | 7.03E-7 Ω·m Show Material materials with Resistividad eléctrica of 7.03E-7 Ω·m | |
600.0 °C | 8.25E-7 Ω·m Show Material materials with Resistividad eléctrica of 8.25E-7 Ω·m | |
Chemical properties
Property | Value |
---|---|
Azufre | 0.01 - 0.025 % Show Material materials with Azufre of 0.01 - 0.025 % |
Carbono | 0.08 - 0.14 % Show Material materials with Carbono of 0.08 - 0.14 % |
Cobre | 0.3 % Show Material materials with Cobre of 0.3 % |
Cromo | 2 - 2.5 % Show Material materials with Cromo of 2 - 2.5 % |
Fósforo | 0.02 - 0.03 % Show Material materials with Fósforo of 0.02 - 0.03 % |
Manganeso | 0.4 - 0.8 % Show Material materials with Manganeso of 0.4 - 0.8 % |
Molibdeno | 0.9 - 1.1 % Show Material materials with Molibdeno of 0.9 - 1.1 % |
Nitrógeno | 0.01 % Show Material materials with Nitrógeno of 0.01 % |