General
Property | Value | Comment |
---|---|---|
Densidad | 2.75 - 2.84 g/cm³ Show Material materials with Densidad of 2.75 - 2.84 g/cm³ | Typical for Wrought 2000 Series Aluminium |
Mecánica
Property | Value | Condition | Related Standards | Comment |
---|---|---|---|---|
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Wrought 2000 Series Aluminium | ||
Elongación | 12.0 % Show Material materials with Elongación of 12.0 % | T4 | JIS H4040 | |
Límite elástico | 245.0 MPa Show Material materials with Límite elástico of 245.0 MPa | T4 | JIS H4040 | |
Módulo de cizallamiento | 26.0 - 27.5 GPa Show Material materials with Módulo de cizallamiento of 26.0 - 27.5 GPa | Typical for Wrought 2000 Series Aluminium | ||
Módulo elástico | 70.0 - 73.0 GPa Show Material materials with Módulo elástico of 70.0 - 73.0 GPa | Typical for Wrought 2000 Series Aluminium | ||
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 2000 Series Aluminium | ||
Resistencia a la tracción | 343.0 MPa Show Material materials with Resistencia a la tracción of 343.0 MPa | T4 | JIS H4040 |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Calor específico | 816.0 - 963.0 J/(kg·K) Show Material materials with Calor específico of 816.0 - 963.0 J/(kg·K) | Typical for Wrought 2000 Series Aluminium |
Coeficiente de dilatación térmica | 1.6e-05 - 2.4e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 1.6e-05 - 2.4e-05 1/K | Typical for Wrought 2000 Series Aluminium |
Conductividad térmica | 112.0 - 251.0 W/(m·K) Show Material materials with Conductividad térmica of 112.0 - 251.0 W/(m·K) | Typical for Wrought 2000 Series Aluminium |
Temperatura de fusión | 500.0 - 650.0 °C Show Material materials with Temperatura de fusión of 500.0 - 650.0 °C | Typical for Wrought 2000 Series Aluminium |
Eléctrico
Property | Value | Comment |
---|---|---|
Conductividad eléctrica | 18000000.0 - 30000000.0 S/m Show Material materials with Conductividad eléctrica of 18000000.0 - 30000000.0 S/m | Typical for Wrought 2000 Series Aluminium |
Resistividad eléctrica | 3.4e-08 - 6e-08 Ω·m Show Material materials with Resistividad eléctrica of 3.4e-08 - 6e-08 Ω·m | Typical for Wrought 2000 Series Aluminium |
Technological properties
Property | ||
---|---|---|
Processing history | T4 | |
Workability | Moderate Workability |