General
Property | Value | Comment |
---|---|---|
Densidad | 2.72 - 2.73 g/cm³ Show Material materials with Densidad of 2.72 - 2.73 g/cm³ | Typical for Wrought 3000 Series Aluminium |
Mecánica
Property | Value | Condition | Related Standards | Comment |
---|---|---|---|---|
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Wrought 3000 Series Aluminium | ||
Elongación | 2.0 % Show Material materials with Elongación of 2.0 % | annealed at 3/4 hard | JIS H4001 | |
Límite elástico | 167.0 MPa Show Material materials with Límite elástico of 167.0 MPa | annealed at 3/4 hard | JIS H4001 | |
Módulo de cizallamiento | 25.0 - 26.0 GPa Show Material materials with Módulo de cizallamiento of 25.0 - 26.0 GPa | Typical for Wrought 3000 Series Aluminium | ||
Módulo elástico | 69.5 - 70.0 GPa Show Material materials with Módulo elástico of 69.5 - 70.0 GPa | Typical for Wrought 3000 Series Aluminium | ||
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 3000 Series Aluminium | ||
Resistencia a la tracción | 196.0 MPa Show Material materials with Resistencia a la tracción of 196.0 MPa | annealed at 3/4 hard | JIS H4001 |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Calor específico | 893.0 - 920.0 J/(kg·K) Show Material materials with Calor específico of 893.0 - 920.0 J/(kg·K) | Typical for Wrought 3000 Series Aluminium |
Coeficiente de dilatación térmica | 2.2e-05 - 2.4e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.2e-05 - 2.4e-05 1/K | Typical for Wrought 3000 Series Aluminium |
Conductividad térmica | 154.0 - 193.0 W/(m·K) Show Material materials with Conductividad térmica of 154.0 - 193.0 W/(m·K) | Typical for Wrought 3000 Series Aluminium |
Temperatura de fusión | 629.0 - 654.0 °C Show Material materials with Temperatura de fusión of 629.0 - 654.0 °C | Typical for Wrought 3000 Series Aluminium |
Eléctrico
Property | Value | Comment |
---|---|---|
Conductividad eléctrica | 23000000.0 - 29000000.0 S/m Show Material materials with Conductividad eléctrica of 23000000.0 - 29000000.0 S/m | Typical for Wrought 3000 Series Aluminium |
Resistividad eléctrica | 3.4e-08 - 4.2e-08 Ω·m Show Material materials with Resistividad eléctrica of 3.4e-08 - 4.2e-08 Ω·m | Typical for Wrought 3000 Series Aluminium |
Technological properties
Property | ||
---|---|---|
Workability | Good workability. |