Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Vickers | 20.0 °C | 200 - 450 [-] Show Material materials with Dureza Vickers of 200 - 450 [-] |
Elongación A5 | 20.0 °C | 5 - 20 % Show Material materials with Elongación A5 of 5 - 20 % |
Resistencia a la tracción | 20.0 °C | 1030 - 1420 MPa Show Material materials with Resistencia a la tracción of 1030 - 1420 MPa |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.75 - 1.5 % Show Material materials with Aluminio of 0.75 - 1.5 % |
Azufre | 0.03 % Show Material materials with Azufre of 0.03 % |
Carbono | 0.09 % Show Material materials with Carbono of 0.09 % |
Cromo | 16 - 18 % Show Material materials with Cromo of 16 - 18 % |
Fósforo | 0.04 % Show Material materials with Fósforo of 0.04 % |
Hierro | 70.59 - 76.75 % Show Material materials with Hierro of 70.59 - 76.75 % |
Manganeso | 1 % Show Material materials with Manganeso of 1 % |
Níquel | 6.5 - 7.75 % Show Material materials with Níquel of 6.5 - 7.75 % |
Silicona | 1 % Show Material materials with Silicona of 1 % |
Technological properties
Property | ||
---|---|---|
Processing history | as cold-rolled, or either as solution-treated or as annealed |