General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.8 g/cm³ Show Material materials with Densidad of 7.8 g/cm³ | Typical for Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Steel |
Dureza Vickers | 23.0 °C | 34 - 530 [-] Show Material materials with Dureza Vickers of 34 - 530 [-] | |
Límite elástico Rp 0,2 | 23.0 °C | 880 - 1320 MPa Show Material materials with Límite elástico Rp 0,2 of 880 - 1320 MPa | |
Módulo elástico | 23.0 °C | 190 - 210 GPa Show Material materials with Módulo elástico of 190 - 210 GPa | Typical for Steel |
Resistencia a la tracción | 23.0 °C | 1140 - 1720 MPa Show Material materials with Resistencia a la tracción of 1140 - 1720 MPa |
Technological properties
Property | ||
---|---|---|
Processing history | as precipitation-hardened |