JIS Z3263 Grade BA11PC H12

Want to keep this datasheet? Save it now in your required format

Description

Aluminum JIS BA11PC is a popular alloy that offers customers very good atmospheric corrosion resistance and moderate strength. Aluminum 3003 offers good machinability for aluminum alloys, though it is not heat treatable. Unlike other aluminum alloys, JIS BA11PC is weldable by conventional welding methods. It also takes cold and hot working well and has generally better mechanical properties when compared to 1000 series aluminum alloys.

Related Standards

Equivalent Materials

Los datos sobre este material han sido proporcionados por Japanese Industrial Standards.

A menos que se indique lo contrario, todas las medidas corresponden a condiciones de temperatura ambiente. A menos que se indique lo contrario, se utilizan las unidades del SI.
Las normas armonizadas son similares a uno o varios estándares del proveedor. Es posible que algunas normas armonizadas se ajusten al estándar original, mientras que otras pueden quedar fuera de su alcance.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Propiedades

General

PropertyValueComment

Densidad

2.72 - 2.73 g/cm³

Show Material materials with Densidad of 2.72 - 2.73 g/cm³

Typical for Wrought 3000 Series Aluminium

Mecánica

PropertyValueConditionRelated StandardsComment

Coeficiente de Poisson

0.33 [-]

Show Material materials with Coeficiente de Poisson of 0.33 [-]

Typical for Wrought 3000 Series Aluminium

Elongación

2.0 %

Show Material materials with Elongación of 2.0 %

H12

JIS Z3263

Módulo de cizallamiento

25.0 - 26.0 GPa

Show Material materials with Módulo de cizallamiento of 25.0 - 26.0 GPa

Typical for Wrought 3000 Series Aluminium

Módulo elástico

69.5 - 70.0 GPa

Show Material materials with Módulo elástico of 69.5 - 70.0 GPa

Typical for Wrought 3000 Series Aluminium

Plane-Strain Fracture Toughnes

22.0 - 35.0 MPa·√m

Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m

Typical for Wrought 3000 Series Aluminium

Resistencia a la tracción

118.0 MPa

Show Material materials with Resistencia a la tracción of 118.0 MPa

H12

JIS Z3263

Aplicaciones térmicas

PropertyValueComment

Calor específico

893.0 - 920.0 J/(kg·K)

Show Material materials with Calor específico of 893.0 - 920.0 J/(kg·K)

Typical for Wrought 3000 Series Aluminium

Coeficiente de dilatación térmica

2.2e-05 - 2.4e-05 1/K

Show Material materials with Coeficiente de dilatación térmica of 2.2e-05 - 2.4e-05 1/K

Typical for Wrought 3000 Series Aluminium

Conductividad térmica

154.0 - 193.0 W/(m·K)

Show Material materials with Conductividad térmica of 154.0 - 193.0 W/(m·K)

Typical for Wrought 3000 Series Aluminium

Temperatura de fusión

629.0 - 654.0 °C

Show Material materials with Temperatura de fusión of 629.0 - 654.0 °C

Typical for Wrought 3000 Series Aluminium

Eléctrico

PropertyValueComment

Conductividad eléctrica

23000000.0 - 29000000.0 S/m

Show Material materials with Conductividad eléctrica of 23000000.0 - 29000000.0 S/m

Typical for Wrought 3000 Series Aluminium

Resistividad eléctrica

3.4e-08 - 4.2e-08 Ω·m

Show Material materials with Resistividad eléctrica of 3.4e-08 - 4.2e-08 Ω·m

Typical for Wrought 3000 Series Aluminium

Technological properties

Property
Processing history

H12

Workability

Good workability.