Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell | 23.0 °C | 207 [-] Show Material materials with Dureza Brinell of 207 [-] |
Dureza Rockwell B | 23.0 °C | 96 [-] Show Material materials with Dureza Rockwell B of 96 [-] |
Dureza Vickers | 23.0 °C | 214 [-] Show Material materials with Dureza Vickers of 214 [-] |
Elongación A5 | 23.0 °C | 30 % Show Material materials with Elongación A5 of 30 % |
Límite elástico Rp 0,2 | 23.0 °C | 235 MPa Show Material materials with Límite elástico Rp 0,2 of 235 MPa |
Resistencia a la tracción | 23.0 °C | 580 MPa Show Material materials with Resistencia a la tracción of 580 MPa |
Technological properties
Property | ||
---|---|---|
Processing history | solution treated |