Property | Value | Comment |
---|---|---|
Densidad | 2.75 - 2.8 g/cm³ Show Material materials with Densidad of 2.75 - 2.8 g/cm³ | Typical for Cast 2xx.x Series Aluminium |
Mecánica
Property | Value | Condition | Related Standards | Comment |
---|---|---|---|---|
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Cast 2xx.x Series Aluminium | ||
Módulo elástico | 72.0 GPa Show Material materials with Módulo elástico of 72.0 GPa | Typical for Cast 2xx.x Series Aluminium | ||
Resistencia a la tracción | 196.0 MPa Show Material materials with Resistencia a la tracción of 196.0 MPa | tempered | JIS H5202 |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Calor específico | 875.0 - 963.0 J/(kg·K) Show Material materials with Calor específico of 875.0 - 963.0 J/(kg·K) | Typical for Cast 2xx.x Series Aluminium |
Coeficiente de dilatación térmica | 1.9e-05 - 2.3e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 1.9e-05 - 2.3e-05 1/K | Typical for Cast 2xx.x Series Aluminium |
Conductividad térmica | 120.0 - 150.0 W/(m·K) Show Material materials with Conductividad térmica of 120.0 - 150.0 W/(m·K) | Typical for Cast 2xx.x Series Aluminium |
Temperatura de fusión | 510.0 - 790.0 °C Show Material materials with Temperatura de fusión of 510.0 - 790.0 °C | Typical for Cast 2xx.x Series Aluminium |
Eléctrico
Property | Value | Comment |
---|---|---|
Conductividad eléctrica | 16000000.0 - 23000000.0 S/m Show Material materials with Conductividad eléctrica of 16000000.0 - 23000000.0 S/m | Typical for Cast 2xx.x Series Aluminium |
Resistividad eléctrica | 4.347826086956522e-08 - 6.25e-08 Ω·m Show Material materials with Resistividad eléctrica of 4.347826086956522e-08 - 6.25e-08 Ω·m | Typical for Cast 2xx.x Series Aluminium |