General
Property | Value | Comment |
---|---|---|
Densidad | 2.6 - 2.7 g/cm³ Show Material materials with Densidad of 2.6 - 2.7 g/cm³ | Typical for Cast 5xx.x Series Aluminium |
Mecánica
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Cast 5xx.x Series Aluminium | |||
Elongación | 12.0 % Show Material materials with Elongación of 12.0 % | as-cast | JIS H5202 | Casting | |
Módulo elástico | 68.0 - 70.0 GPa Show Material materials with Módulo elástico of 68.0 - 70.0 GPa | Typical for Cast 5xx.x Series Aluminium | |||
Resistencia a la tracción | 216.0 MPa Show Material materials with Resistencia a la tracción of 216.0 MPa | as-cast | JIS H5202 | Casting |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Calor específico | 963.0 J/(kg·K) Show Material materials with Calor específico of 963.0 J/(kg·K) | Typical for Cast 5xx.x Series Aluminium |
Coeficiente de dilatación térmica | 2.3e-05 - 2.5e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.3e-05 - 2.5e-05 1/K | Typical for Cast 5xx.x Series Aluminium |
Conductividad térmica | 60.0 - 140.0 W/(m·K) Show Material materials with Conductividad térmica of 60.0 - 140.0 W/(m·K) | Typical for Cast 5xx.x Series Aluminium |
Temperatura de fusión | 450.0 - 640.0 °C Show Material materials with Temperatura de fusión of 450.0 - 640.0 °C | Typical for Cast 5xx.x Series Aluminium |