General
Property | Value | Comment |
---|---|---|
Densidad | 7.8 g/cm³ Show Material materials with Densidad of 7.8 g/cm³ | Typical for Steel |
Mecánica
Property | Value | Comment |
---|---|---|
Coeficiente de Poisson | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Steel |
Elongación | 14.1 % Show Material materials with Elongación of 14.1 % | Predicted Value, A200 |
15.5 % Show Material materials with Elongación of 15.5 % | Predicted Value, A80 | |
17.5 % Show Material materials with Elongación of 17.5 % | Predicted Value, Transverse | |
20.2 % Show Material materials with Elongación of 20.2 % | Predicted Value, A80 Transverse | |
20.3 % Show Material materials with Elongación of 20.3 % | Predicted Value, A5 | |
21.1 % Show Material materials with Elongación of 21.1 % | Predicted Value, A50 | |
21.7 % Show Material materials with Elongación of 21.7 % | Predicted Value | |
Estricción | 41.2 % Show Material materials with Estricción of 41.2 % | Predicted Value |
42.9 % Show Material materials with Estricción of 42.9 % | Predicted Value, Transverse | |
Módulo de cizallamiento | 79.4 GPa Show Material materials with Módulo de cizallamiento of 79.4 GPa | Predicted Value |
Módulo elástico | 190 - 210 GPa Show Material materials with Módulo elástico of 190 - 210 GPa | Typical for Steel |
Resistencia al cizallamiento | 515 MPa Show Material materials with Resistencia al cizallamiento of 515 MPa | Predicted Value |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Calor específico | 461.8 J/(kg·K) Show Material materials with Calor específico of 461.8 J/(kg·K) | Predicted Value |
Coeficiente de dilatación térmica | 11.78 1/K Show Material materials with Coeficiente de dilatación térmica of 11.78 1/K | Predicted Value |
Conductividad térmica | 40.42 W/(m·K) Show Material materials with Conductividad térmica of 40.42 W/(m·K) | Predicted Value |
Eléctrico
Chemical properties
Property | Value | Related Standards |
---|---|---|
Azufre | 0.03 % Show Material materials with Azufre of 0.03 % | ASTM A572 |
Carbono | 0.26 % Show Material materials with Carbono of 0.26 % | ASTM A572 |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % | ASTM A572 |
Manganeso | 1.35 % Show Material materials with Manganeso of 1.35 % | ASTM A572 |
Silicona | 0.4 % Show Material materials with Silicona of 0.4 % | ASTM A572 |
Technological properties
Property | ||
---|---|---|
Supplier Disclaimer | The given information is a rough description and some properties can depend on various factors such as product thickness. Please contact the supplier or refer to the related norm or standard for further information. |