Medium Carbon Steel
EN 10028-3 Grade P355N normalized or normalized formed (+N)Suministrada por:
2 proveedores de Matmatch
Unclassified Low Alloy Steel
EN 10028-6 Grade P690QL1 quenched and tempered (+QT)Suministrada por:
1 proveedor Matmatch
Unclassified Low Alloy Steel
EN 10028-6 Grade P690QL2 quenched and tempered (+QT)Suministrada por:
1 proveedor Matmatch
Medium Carbon Steel
EN 10083-3 Grade 30MnB5 quenched and tempered (+QT)Suministrada por:
1 proveedor Matmatch
Nickel Molybdenum Steel
ASTM A387 Grade 11 Class 1, Annealed, Normalized and Tempered, or Quenched and TemperedSuministrada por:
1 proveedor Matmatch
Unclassified Carbon Steel
ASTM A516 Grade 380 As-Rolled or Normalized and/or Stress RelievedSuministrada por:
1 proveedor Matmatch
Chromium Molybdenum Steel
ASTM A542 Type D Class 1 Quenched and TemperedSuministrada por:
1 proveedor Matmatch
Unclassified Stainless Steel
ASTM A543 Class 1 Type C Quenched and TemperedSuministrada por:
1 proveedor Matmatch
Unclassified Carbon Steel
ASTM A516 Grade 415 As-Rolled or Normalized and/or Stress RelievedSuministrada por:
1 proveedor Matmatch
Medium Carbon Steel
DIN 1629 Grade St 52.0 normalized or normalized formed (+N)Medium Carbon Steel
EN 10250-2 Grade C55 normalized and tempered (+NT)Medium Carbon Steel
EN 10216-3 Grade P355N normalized or normalized formed (+N)Medium Carbon Steel
EN 10250-2 Grade C35 normalized and tempered (+NT)Medium Carbon Steel
EN 10250-2 Grade C35E normalized and tempered (+NT)Medium Carbon Steel
EN 10250-2 Grade C35E normalized or normalized formed (+N)Medium Carbon Steel
EN 10250-2 Grade C45E normalized and tempered (+NT)Medium Carbon Steel
EN 10250-2 Grade C45E normalized or normalized formed (+N)