General
Property | Value | Comment |
---|---|---|
Densidad | 7.8 g/cm³ Show Material materials with Densidad of 7.8 g/cm³ | Typical for Steel |
Mecánica
Property | Value | Related Standards | Shape | Comment |
---|---|---|---|---|
Coeficiente de Poisson | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Steel | ||
Elongación | 17.5 % Show Material materials with Elongación of 17.5 % | Predicted Value, A80 | ||
18 % Show Material materials with Elongación of 18 % | ASTM A573 | Plate | A200 | |
18.1 % Show Material materials with Elongación of 18.1 % | Predicted Value, Transverse | |||
19.3 % Show Material materials with Elongación of 19.3 % | Predicted Value, A80 Transverse | |||
21 % Show Material materials with Elongación of 21 % | ASTM A573 | Plate | A50 | |
23.1 % Show Material materials with Elongación of 23.1 % | Predicted Value | |||
Estricción | 43.6 % Show Material materials with Estricción of 43.6 % | Predicted Value, Transverse | ||
43.8 % Show Material materials with Estricción of 43.8 % | Predicted Value | |||
Límite elástico | 265.5 MPa Show Material materials with Límite elástico of 265.5 MPa | Predicted Value, RP1 | ||
288.6 MPa Show Material materials with Límite elástico of 288.6 MPa | Predicted Value, RP05 | |||
290 MPa Show Material materials with Límite elástico of 290 MPa | ASTM A573 | Plate | ||
315.9 MPa Show Material materials with Límite elástico of 315.9 MPa | Predicted Value, RP1 Transverse | |||
329 MPa Show Material materials with Límite elástico of 329 MPa | Predicted Value, Transverse | |||
372.1 MPa Show Material materials with Límite elástico of 372.1 MPa | Predicted Value, RP02 | |||
411.9 MPa Show Material materials with Límite elástico of 411.9 MPa | Predicted Value, RP002 | |||
484.2 MPa Show Material materials with Límite elástico of 484.2 MPa | Predicted Value, RP02 Transverse | |||
Módulo de cizallamiento | 79.4 GPa Show Material materials with Módulo de cizallamiento of 79.4 GPa | Predicted Value | ||
Módulo elástico | 190 - 210 GPa Show Material materials with Módulo elástico of 190 - 210 GPa | Typical for Steel | ||
Resistencia a la tracción | 485 - 620 MPa Show Material materials with Resistencia a la tracción of 485 - 620 MPa | ASTM A573 | Plate | |
Resistencia al cizallamiento | 534.7 MPa Show Material materials with Resistencia al cizallamiento of 534.7 MPa | Predicted Value |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Calor específico | 459.7 J/(kg·K) Show Material materials with Calor específico of 459.7 J/(kg·K) | Predicted Value |
Coeficiente de dilatación térmica | 12.1 1/K Show Material materials with Coeficiente de dilatación térmica of 12.1 1/K | Predicted Value |
Conductividad térmica | 38.44 W/(m·K) Show Material materials with Conductividad térmica of 38.44 W/(m·K) | Predicted Value |
Eléctrico
Chemical properties
Property | Value | Related Standards | Shape |
---|---|---|---|
Azufre | 0.03 % Show Material materials with Azufre of 0.03 % | ASTM A573 | Plate |
Carbono | 0.27 % Show Material materials with Carbono of 0.27 % | ASTM A573 | Plate |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % | ASTM A573 | Plate |
Manganeso | 0.85 - 1.2 % Show Material materials with Manganeso of 0.85 - 1.2 % | ASTM A573 | Plate |
Silicona | 0.15 - 0.4 % Show Material materials with Silicona of 0.15 - 0.4 % | ASTM A573 | Plate |