General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 20.0 °C | 7.8 - 7.9 g/cm³ Show Material materials with Densidad of 7.8 - 7.9 g/cm³ | Typical for Nickel Chromium Molybdenum Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 20.0 °C | 0.29 [-] Show Material materials with Coeficiente de Poisson of 0.29 [-] | Typical for Nickel Chromium Molybdenum Steel |
Dureza Brinell | 20.0 °C | 207 [-] Show Material materials with Dureza Brinell of 207 [-] | |
Elongación A50 | 20.0 °C | 20 % Show Material materials with Elongación A50 of 20 % | |
Módulo elástico | 20.0 °C | 200 - 215 GPa Show Material materials with Módulo elástico of 200 - 215 GPa | Typical for Nickel Chromium Molybdenum Steel |
Resistencia a la tracción | 20.0 °C | 690 - 860 MPa Show Material materials with Resistencia a la tracción of 690 - 860 MPa | |
Yield Strength Rp0.2, short transverse | 20.0 °C | 550 MPa Show Material materials with Yield Strength Rp0.2, short transverse of 550 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 20.0 °C | 1E-5 - 1.3E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1E-5 - 1.3E-5 1/K | Typical for Nickel Chromium Molybdenum Steel |
Conductividad térmica | 20.0 °C | 34 - 54 W/(m·K) Show Material materials with Conductividad térmica of 34 - 54 W/(m·K) | Typical for Nickel Chromium Molybdenum Steel |
Temperatura de fusión | 1382 - 1529 °C Show Material materials with Temperatura de fusión of 1382 - 1529 °C | Typical for Nickel Chromium Molybdenum Steel |
Chemical properties
Property | Value |
---|---|
Azufre | 0.01 % Show Material materials with Azufre of 0.01 % |
Carbono | 0.18 % Show Material materials with Carbono of 0.18 % |
Cromo | 1 - 1.8 % Show Material materials with Cromo of 1 - 1.8 % |
Fósforo | 0.02 % Show Material materials with Fósforo of 0.02 % |
Manganeso | 0.1 - 0.4 % Show Material materials with Manganeso of 0.1 - 0.4 % |
Molibdeno | 0.2 - 0.6 % Show Material materials with Molibdeno of 0.2 - 0.6 % |
Níquel | 2 - 3.3 % Show Material materials with Níquel of 2 - 3.3 % |
Silicona | 0.15 - 0.35 % Show Material materials with Silicona of 0.15 - 0.35 % |