Yield Strength Rp0.2, short transverse: 550 MPa

Quick Comparison

Acero inoxidable martensítico

ASTM A487 Grade 6 Class A, Heat-Treated

Acero inoxidable martensítico

ASTM A487 Grade CA6NM Class A, Heat-Treated

Chromium Molybdenum Steel

ASTM A193 Grade B5 Up to M100, incl

Acero inoxidable martensítico

ASTM A487 Grade CA6NM Class A, Heat-Treated

Acero inoxidable martensítico

ASTM A487 Grade 7 Class A, Heat-Treated

Nickel Chromium Molybdenum Steel

ASTM A487 Grade 14 Class A, Heat-Treated

Nickel Chromium Molybdenum Steel

ASTM A487 Grade 10 Class B, Heat-Treated

Nickel Chromium Molybdenum Steel

ASTM A487 Grade 12 Class B, Heat-Treated

Nickel Chromium Molybdenum Steel

ASTM A487 Grade 13 Class B, Heat-Treated
Página 1 de 2