Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.8 g/cm³ Show Material materials with Densidad of 7.8 g/cm³ | Typical for Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Steel |
Dureza Brinell | 23.0 °C | 277 [-] Show Material materials with Dureza Brinell of 277 [-] | |
Elongación A50 | 23.0 °C | 15 % Show Material materials with Elongación A50 of 15 % | |
Energía de impacto Charpy | 23.0 °C | 27 J Show Material materials with Energía de impacto Charpy of 27 J | |
Estricción | 23.0 °C | 50 % Show Material materials with Estricción of 50 % | |
Límite elástico Rp 0,2 | 23.0 °C | 515 MPa Show Material materials with Límite elástico Rp 0,2 of 515 MPa | |
Módulo elástico | 23.0 °C | 190 - 210 GPa Show Material materials with Módulo elástico of 190 - 210 GPa | Typical for Steel |
Resistencia a la tracción | 23.0 °C | 795 MPa Show Material materials with Resistencia a la tracción of 795 MPa |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.05 % Show Material materials with Aluminio of 0.05 % |
Azufre | 0.03 % Show Material materials with Azufre of 0.03 % |
Carbono | 0.13 - 0.18 % Show Material materials with Carbono of 0.13 - 0.18 % |
Cromo | 11.5 - 13 % Show Material materials with Cromo of 11.5 - 13 % |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % |
Manganeso | 0.4 - 0.6 % Show Material materials with Manganeso of 0.4 - 0.6 % |
Molibdeno | 0.2 % Show Material materials with Molibdeno of 0.2 % |
Niobio | 0.15 - 0.45 % Show Material materials with Niobio of 0.15 - 0.45 % |
Níquel | 0.5 % Show Material materials with Níquel of 0.5 % |
Silicona | 0.5 % Show Material materials with Silicona of 0.5 % |