Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell | 23.0 °C | 170 [-] Show Material materials with Dureza Brinell of 170 [-] |
Dureza Rockwell B | 23.0 °C | 87 [-] Show Material materials with Dureza Rockwell B of 87 [-] |
Elongación A50 | 23.0 °C | 25 % Show Material materials with Elongación A50 of 25 % |
Límite elástico | 23.0 °C | 255 MPa Show Material materials with Límite elástico of 255 MPa |
Resistencia a la tracción | 23.0 °C | 415 MPa Show Material materials with Resistencia a la tracción of 415 MPa |
Chemical properties
Property | Value |
---|---|
Azufre | 0.06 % Show Material materials with Azufre of 0.06 % |
Carbono | 0.15 % Show Material materials with Carbono of 0.15 % |
Cobre | 0.2 - 0.6 % Show Material materials with Cobre of 0.2 - 0.6 % |
Cromo | 0.24 - 1.31 % Show Material materials with Cromo of 0.24 - 1.31 % |
Fósforo | 0.06 - 0.16 % Show Material materials with Fósforo of 0.06 - 0.16 % |
Manganeso | 0.55 % Show Material materials with Manganeso of 0.55 % |
Níquel | 0.2 - 0.7 % Show Material materials with Níquel of 0.2 - 0.7 % |
Silicona | 0.1 % Show Material materials with Silicona of 0.1 % |