Acero bajo en carbono
DIN 2395-3 Grade St 44-2 welded and cold sizedAcero bajo en carbono
DIN 2395-3 Grade St 44-2 normalized or normalized formed (+N)Acero bajo en carbono
DIN 2395-3 Grade St 37-3 welded and cold sizedAcero bajo en carbono
DIN 2395-3 Grade St 37-3 normalized or normalized formed (+N)Acero bajo en carbono
DIN 17111 Grade U 7 S 6 hot rolledAcero de alto carbono
EN 10132-4 Grade C75S Quenched and TemperedNickel Chromium Alloy
WL 2.4630 Grade NiCr20Ti soft annealed (+A)Acero bajo en carbono
DIN 17111 Grade R 7 S 6 hot rolledMedium Carbon Steel
SEW 101 Grade 49MnVS3 hot worked and controlled cooledMalleable Cast Iron
SAE J158 Grade M3210 AnnealedMalleable Cast Iron
SAE J158 Grade M4504 Air quenched and TemperedMalleable Cast Iron
SAE J158 Grade M5003 Air quenched and TemperedMalleable Cast Iron
SAE J158 Grade M5503 Liquid quenched and TemperedMalleable Cast Iron
SAE J158 Grade M7002 Liquid quenched and TemperedMalleable Cast Iron
SAE J158 Grade M8501 Liquid quenched and TemperedAcero bajo en carbono
DIN 17140-1 Grade D 9Acero bajo en carbono
ASTM A183 Grade Nut Reduced-Section Tension TestManganese Steel
SEW 101 Grade 38MnSiVS5 hot worked and controlled cooled