Mecánica
Chemical properties
Property | Value |
---|---|
Azufre | 0.06 % Show Material materials with Azufre of 0.06 % |
Carbono | 2 - 3.3 % Show Material materials with Carbono of 2 - 3.3 % |
Cobre | 1.2 % Show Material materials with Cobre of 1.2 % |
Cromo | 11 - 14 % Show Material materials with Cromo of 11 - 14 % |
Fósforo | 0.1 % Show Material materials with Fósforo of 0.1 % |
Manganeso | 2 % Show Material materials with Manganeso of 2 % |
Molibdeno | 3 % Show Material materials with Molibdeno of 3 % |
Níquel | 2.5 % Show Material materials with Níquel of 2.5 % |
Silicona | 1.5 % Show Material materials with Silicona of 1.5 % |