General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 6.8 - 7.8 g/cm³ Show Material materials with Densidad of 6.8 - 7.8 g/cm³ | Typical for Cast Iron |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.27 [-] Show Material materials with Coeficiente de Poisson of 0.27 [-] | Typical for Cast Iron |
Dureza Brinell | 23.0 °C | 450 [-] Show Material materials with Dureza Brinell of 450 [-] | |
Dureza Rockwell C | 23.0 °C | 46 [-] Show Material materials with Dureza Rockwell C of 46 [-] | |
Dureza Vickers | 23.0 °C | 485 [-] Show Material materials with Dureza Vickers of 485 [-] | |
Módulo de cizallamiento | 23.0 °C | 41 GPa Show Material materials with Módulo de cizallamiento of 41 GPa | Typical for Cast Iron |
Módulo elástico | 23.0 °C | 152 GPa Show Material materials with Módulo elástico of 152 GPa | Typical for Cast Iron |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 460 - 527 J/(kg·K) Show Material materials with Calor específico of 460 - 527 J/(kg·K) | Typical for Cast Iron |
Conductividad térmica | 23.0 °C | 55 W/(m·K) Show Material materials with Conductividad térmica of 55 W/(m·K) | Typical for Cast Iron |
Temperatura de fusión | 1120 °C Show Material materials with Temperatura de fusión of 1120 °C | Typical for Cast Iron |
Chemical properties
Property | Value |
---|---|
Azufre | 0.06 % Show Material materials with Azufre of 0.06 % |
Carbono | 2 - 3.3 % Show Material materials with Carbono of 2 - 3.3 % |
Cobre | 1.2 % Show Material materials with Cobre of 1.2 % |
Cromo | 18 - 23 % Show Material materials with Cromo of 18 - 23 % |
Fósforo | 0.1 % Show Material materials with Fósforo of 0.1 % |
Manganeso | 2 % Show Material materials with Manganeso of 2 % |
Molibdeno | 3 % Show Material materials with Molibdeno of 3 % |
Níquel | 2.5 % Show Material materials with Níquel of 2.5 % |
Silicona | 1 - 2.2 % Show Material materials with Silicona of 1 - 2.2 % |