Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.8 - 7.9 g/cm³ Show Material materials with Densidad of 7.8 - 7.9 g/cm³ | Typical for Nickel Chromium Molybdenum Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.29 [-] Show Material materials with Coeficiente de Poisson of 0.29 [-] | Typical for Nickel Chromium Molybdenum Steel |
Elongación A50 | 23.0 °C | 5 % Show Material materials with Elongación A50 of 5 % | |
Límite elástico | 23.0 °C | 1000 MPa Show Material materials with Límite elástico of 1000 MPa | |
Módulo elástico | 23.0 °C | 200 - 215 GPa Show Material materials with Módulo elástico of 200 - 215 GPa | Typical for Nickel Chromium Molybdenum Steel |
Resistencia a la tracción | 23.0 °C | 1241 MPa Show Material materials with Resistencia a la tracción of 1241 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 448 - 670 J/(kg·K) Show Material materials with Calor específico of 448 - 670 J/(kg·K) | Typical for Nickel Chromium Molybdenum Steel |
Coeficiente de dilatación térmica | 23.0 °C | 1E-5 - 1.3E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1E-5 - 1.3E-5 1/K | Typical for Nickel Chromium Molybdenum Steel |
Conductividad térmica | 23.0 °C | 34 - 54 W/(m·K) Show Material materials with Conductividad térmica of 34 - 54 W/(m·K) | Typical for Nickel Chromium Molybdenum Steel |
Temperatura de fusión | 1382 - 1529 °C Show Material materials with Temperatura de fusión of 1382 - 1529 °C | Typical for Nickel Chromium Molybdenum Steel |
Chemical properties
Property | Value |
---|---|
Azufre | 0.045 % Show Material materials with Azufre of 0.045 % |
Carbono | 0.35 - 0.45 % Show Material materials with Carbono of 0.35 - 0.45 % |
Cromo | 0.7 - 0.9 % Show Material materials with Cromo of 0.7 - 0.9 % |
Fósforo | 0.04 % Show Material materials with Fósforo of 0.04 % |
Manganeso | 0.7 - 1 % Show Material materials with Manganeso of 0.7 - 1 % |
Molibdeno | 0.2 - 0.3 % Show Material materials with Molibdeno of 0.2 - 0.3 % |
Níquel | 1.65 - 2 % Show Material materials with Níquel of 1.65 - 2 % |
Silicona | 0.2 - 0.8 % Show Material materials with Silicona of 0.2 - 0.8 % |