Níquel: 1.65 - 2 %

Quick Comparison

Nickel Steel

EN 10028-4 Grade 15NiMn6 normalized or normalized formed (+N)

Suministrada por:

1 proveedor Matmatch

Unclassified Low Alloy Steel

EN 10025-6 Grade S550QL1 quenched and tempered (+QT)

Suministrada por:

1 proveedor Matmatch

Unclassified Low Alloy Steel

EN 10025-6 Grade S620QL1 quenched and tempered (+QT)

Suministrada por:

1 proveedor Matmatch

Unclassified Low Alloy Steel

EN 10025-6 Grade S690QL1 quenched and tempered (+QT)

Suministrada por:

1 proveedor Matmatch

Unclassified Low Alloy Steel

EN 10025-6 Grade S460Q quenched and tempered (+QT)

Suministrada por:

1 proveedor Matmatch

Unclassified Low Alloy Steel

EN 10025-6 Grade S460QL quenched and tempered (+QT)

Suministrada por:

1 proveedor Matmatch

Unclassified Low Alloy Steel

EN 10025-6 Grade S460QL1 quenched and tempered (+QT)

Suministrada por:

1 proveedor Matmatch

Unclassified Low Alloy Steel

EN 10025-6 Grade S500Q quenched and tempered (+QT)

Suministrada por:

1 proveedor Matmatch

Unclassified Low Alloy Steel

EN 10025-6 Grade S500QL quenched and tempered (+QT)

Suministrada por:

1 proveedor Matmatch

Unclassified Low Alloy Steel

EN 10025-6 Grade S500QL1 quenched and tempered (+QT)

Suministrada por:

1 proveedor Matmatch

Unclassified Low Alloy Steel

EN 10025-6 Grade S550Q quenched and tempered (+QT)

Suministrada por:

1 proveedor Matmatch

Unclassified Low Alloy Steel

EN 10025-6 Grade S550QL quenched and tempered (+QT)

Suministrada por:

1 proveedor Matmatch

Unclassified Low Alloy Steel

EN 10025-6 Grade S620Q quenched and tempered (+QT)

Suministrada por:

1 proveedor Matmatch

Unclassified Low Alloy Steel

EN 10025-6 Grade S620QL quenched and tempered (+QT)

Suministrada por:

1 proveedor Matmatch

Unclassified Low Alloy Steel

EN 10025-6 Grade S690Q quenched and tempered (+QT)

Suministrada por:

1 proveedor Matmatch

Unclassified Low Alloy Steel

EN 10025-6 Grade S690QL quenched and tempered (+QT)

Suministrada por:

1 proveedor Matmatch

Unclassified Low Alloy Steel

EN 10025-6 Grade S960Q quenched and tempered (+QT)

Suministrada por:

1 proveedor Matmatch

Wrought Copper Nickel Grade

UNS C70260 boway

Suministrada por:

Ningbo Boway Alloy Material

Wrought Copper High Copper Alloy

ASTM B768 Grade C17510 TH04

Wrought Copper High Copper Alloy

ASTM B768 Grade C17510 TF00
Página 1 de 42