General
Property | Value | Comment |
---|---|---|
Densidad | 7.8 - 7.9 g/cm³ Show Material materials with Densidad of 7.8 - 7.9 g/cm³ | Typical for Low Carbon Steel |
Mecánica
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Coeficiente de Poisson | 0.29 [-] Show Material materials with Coeficiente de Poisson of 0.29 [-] | Typical for Low Carbon Steel | |||
Dureza Brinell | 262 [-] Show Material materials with Dureza Brinell of 262 [-] | Predicted Value, Transverse | |||
Elongación | 16.7 % Show Material materials with Elongación of 16.7 % | Predicted Value, A200 | |||
19.0 % Show Material materials with Elongación of 19.0 % | Predicted Value, Transverse | ||||
19.5 % Show Material materials with Elongación of 19.5 % | Predicted Value, A80 | ||||
20 % Show Material materials with Elongación of 20 % | Quenched and Tempered | ASTM A203 | Plate | A50 | |
20.8 % Show Material materials with Elongación of 20.8 % | Predicted Value, A80 Transverse | ||||
21.8 % Show Material materials with Elongación of 21.8 % | Predicted Value | ||||
Estricción | 43.1 % Show Material materials with Estricción of 43.1 % | Predicted Value | |||
43.6 % Show Material materials with Estricción of 43.6 % | Predicted Value, Transverse | ||||
Límite elástico | 263.2 MPa Show Material materials with Límite elástico of 263.2 MPa | Predicted Value, RP1 | |||
297.6 MPa Show Material materials with Límite elástico of 297.6 MPa | Predicted Value, RP05 | ||||
317.5 MPa Show Material materials with Límite elástico of 317.5 MPa | Predicted Value, RP1 Transverse | ||||
343.2 MPa Show Material materials with Límite elástico of 343.2 MPa | Predicted Value, Transverse | ||||
345 MPa Show Material materials with Límite elástico of 345 MPa | Quenched and Tempered | ASTM A203 | Plate | ||
380 MPa Show Material materials with Límite elástico of 380 MPa | Quenched and Tempered | ASTM A203 | Plate | ||
414.1 MPa Show Material materials with Límite elástico of 414.1 MPa | Predicted Value, RP02 | ||||
473.4 MPa Show Material materials with Límite elástico of 473.4 MPa | Predicted Value, RP002 | ||||
475.8 MPa Show Material materials with Límite elástico of 475.8 MPa | Predicted Value, RP02 Transverse | ||||
Módulo de cizallamiento | 82 GPa Show Material materials with Módulo de cizallamiento of 82 GPa | Typical for Low Carbon Steel | |||
Módulo elástico | 200 - 215 GPa Show Material materials with Módulo elástico of 200 - 215 GPa | Typical for Low Carbon Steel | |||
Resistencia a la tracción | 550 - 690 MPa Show Material materials with Resistencia a la tracción of 550 - 690 MPa | Quenched and Tempered | ASTM A203 | Plate | |
Resistencia al cizallamiento | 526 MPa Show Material materials with Resistencia al cizallamiento of 526 MPa | Predicted Value |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Calor específico | 465 J/(kg·K) Show Material materials with Calor específico of 465 J/(kg·K) | Typical for Low Carbon Steel |
Coeficiente de dilatación térmica | 1.32e-05 - 1.38e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 1.32e-05 - 1.38e-05 1/K | Typical for Low Carbon Steel |
Conductividad térmica | 25 - 93 W/(m·K) Show Material materials with Conductividad térmica of 25 - 93 W/(m·K) | Typical for Low Carbon Steel |
Temperatura de fusión | 1480 - 1526 °C Show Material materials with Temperatura de fusión of 1480 - 1526 °C | Typical for Low Carbon Steel |
Temperatura máx. de funcionamiento | 337.4 °C Show Material materials with Temperatura máx. de funcionamiento of 337.4 °C | Predicted Value, Long |
500 °C Show Material materials with Temperatura máx. de funcionamiento of 500 °C | Typical for Carbon Steel |
Eléctrico
Property | Value | Comment |
---|---|---|
Conductividad eléctrica | 7 S/m Show Material materials with Conductividad eléctrica of 7 S/m | Predicted Value |
Resistividad eléctrica | 1.43e-07 - 1.74e-07 Ω·m Show Material materials with Resistividad eléctrica of 1.43e-07 - 1.74e-07 Ω·m | Typical for Carbon Steel |
Magnético
Property | Value | Comment |
---|---|---|
Temperatura de Curie | 770 °C Show Material materials with Temperatura de Curie of 770 °C | Typical for Low Carbon Steel |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Azufre | 0.8 % Show Material materials with Azufre of 0.8 % | Quenched and Tempered | ASTM A203 | Plate |
Carbono | 0.2 % Show Material materials with Carbono of 0.2 % | Quenched and Tempered | ASTM A203 | Plate |
Fósforo | 0.7 % Show Material materials with Fósforo of 0.7 % | Quenched and Tempered | ASTM A203 | Plate |
Manganeso | 0.7 % Show Material materials with Manganeso of 0.7 % | Quenched and Tempered | ASTM A203 | Plate |
Níquel | 3.25 - 3.75 % Show Material materials with Níquel of 3.25 - 3.75 % | Quenched and Tempered | ASTM A203 | Plate |
Silicona | 0.15 - 0.4 % Show Material materials with Silicona of 0.15 - 0.4 % | Quenched and Tempered | ASTM A203 | Plate |
Technological properties
Property | ||
---|---|---|
Supplier Disclaimer | The given information is a rough description and some properties can depend on various factors such as product thickness. Please contact the supplier or refer to the related norm or standard for further information. |