General
Property | Value | Comment |
---|---|---|
Densidad | 7.8 - 7.9 g/cm³ Show Material materials with Densidad of 7.8 - 7.9 g/cm³ | Typical for Chromium Molybdenum Steel |
Mecánica
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Coeficiente de Poisson | 0.29 [-] Show Material materials with Coeficiente de Poisson of 0.29 [-] | Typical for Chromium Molybdenum Steel | |||
Elongación | 9.8 % Show Material materials with Elongación of 9.8 % | Predicted Value, A200 | |||
14 % Show Material materials with Elongación of 14 % | Quenched and Tempered | ASTM A542 | Plate | A50 | |
16.1 % Show Material materials with Elongación of 16.1 % | Predicted Value, A80 | ||||
18.1 % Show Material materials with Elongación of 18.1 % | Predicted Value, Transverse | ||||
19.7 % Show Material materials with Elongación of 19.7 % | Predicted Value | ||||
19.9 % Show Material materials with Elongación of 19.9 % | Predicted Value, A80 Transverse | ||||
Estricción | 44.3 % Show Material materials with Estricción of 44.3 % | Predicted Value, Transverse | |||
44.5 % Show Material materials with Estricción of 44.5 % | Predicted Value | ||||
Límite elástico | 300.7 MPa Show Material materials with Límite elástico of 300.7 MPa | Predicted Value, RP1 | |||
329.5 MPa Show Material materials with Límite elástico of 329.5 MPa | Predicted Value, RP1 Transverse | ||||
473 MPa Show Material materials with Límite elástico of 473 MPa | Predicted Value, RP05 | ||||
507.8 MPa Show Material materials with Límite elástico of 507.8 MPa | Predicted Value, RP02 Transverse | ||||
511.6 MPa Show Material materials with Límite elástico of 511.6 MPa | Predicted Value, Transverse | ||||
585 MPa Show Material materials with Límite elástico of 585 MPa | Quenched and Tempered | ASTM A542 | Plate | ||
621.7 MPa Show Material materials with Límite elástico of 621.7 MPa | Predicted Value, RP02 | ||||
655.6 MPa Show Material materials with Límite elástico of 655.6 MPa | Predicted Value, RP002 | ||||
Módulo de cizallamiento | 79.4 GPa Show Material materials with Módulo de cizallamiento of 79.4 GPa | Predicted Value | |||
Módulo elástico | 200 - 215 GPa Show Material materials with Módulo elástico of 200 - 215 GPa | Typical for Chromium Molybdenum Steel | |||
Resistencia a la tracción | 725 - 860 MPa Show Material materials with Resistencia a la tracción of 725 - 860 MPa | Quenched and Tempered | ASTM A542 | Plate | |
Resistencia al cizallamiento | 699.7 MPa Show Material materials with Resistencia al cizallamiento of 699.7 MPa | Predicted Value |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Calor específico | 448 - 502 J/(kg·K) Show Material materials with Calor específico of 448 - 502 J/(kg·K) | Typical for Chromium Molybdenum Steel |
Coeficiente de dilatación térmica | 1.1e-05 - 1.4e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 1.1e-05 - 1.4e-05 1/K | Typical for Chromium Molybdenum Steel |
Conductividad térmica | 36 - 43 W/(m·K) Show Material materials with Conductividad térmica of 36 - 43 W/(m·K) | Typical for Chromium Molybdenum Steel |
Temperatura de fusión | 1382 - 1529 °C Show Material materials with Temperatura de fusión of 1382 - 1529 °C | Typical for Chromium Molybdenum Steel |
Eléctrico
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Azufre | 0.01 % Show Material materials with Azufre of 0.01 % | Quenched and Tempered | ASTM A542 | Plate |
Boro | 0.002 % Show Material materials with Boro of 0.002 % | Quenched and Tempered | ASTM A542 | Plate |
Carbono | 0.11 - 0.15 % Show Material materials with Carbono of 0.11 - 0.15 % | Quenched and Tempered | ASTM A542 | Plate |
Cobre | 0.2 % Show Material materials with Cobre of 0.2 % | Quenched and Tempered | ASTM A542 | Plate |
Cromo | 2 - 2.5 % Show Material materials with Cromo of 2 - 2.5 % | Quenched and Tempered | ASTM A542 | Plate |
Fósforo | 0.015 % Show Material materials with Fósforo of 0.015 % | Quenched and Tempered | ASTM A542 | Plate |
Manganeso | 0.3 - 0.6 % Show Material materials with Manganeso of 0.3 - 0.6 % | Quenched and Tempered | ASTM A542 | Plate |
Molibdeno | 0.9 - 1.1 % Show Material materials with Molibdeno of 0.9 - 1.1 % | Quenched and Tempered | ASTM A542 | Plate |
Niobio | 0.07 % Show Material materials with Niobio of 0.07 % | Quenched and Tempered | ASTM A542 | Plate |
Níquel | 0.25 % Show Material materials with Níquel of 0.25 % | Quenched and Tempered | ASTM A542 | Plate |
Silicona | 0.1 % Show Material materials with Silicona of 0.1 % | Quenched and Tempered | ASTM A542 | Plate |
Titanio | 0.03 % Show Material materials with Titanio of 0.03 % | Quenched and Tempered | ASTM A542 | Plate |
Vanadio | 0.25 - 0.35 % Show Material materials with Vanadio of 0.25 - 0.35 % | Quenched and Tempered | ASTM A542 | Plate |
Technological properties
Property | ||
---|---|---|
Supplier Disclaimer | The given information is a rough description and some properties can depend on various factors such as product thickness. Please contact the supplier or refer to the related norm or standard for further information. |