Mecánica
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Energía de impacto Charpy | 27 J Show Material materials with Energía de impacto Charpy of 27 J | Heat-Treated | ASTM A738 | Plate |
Límite elástico | 415 MPa Show Material materials with Límite elástico of 415 MPa | Heat-Treated | ASTM A738 | Plate |
Resistencia a la tracción | 585 - 705 MPa Show Material materials with Resistencia a la tracción of 585 - 705 MPa | Heat-Treated | ASTM A738 | Plate |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Azufre | 0.025 % Show Material materials with Azufre of 0.025 % | Heat-Treated | ASTM A738 | Plate |
Carbono | 0.2 % Show Material materials with Carbono of 0.2 % | Heat-Treated | ASTM A738 | Plate |
Cobre | 0.35 % Show Material materials with Cobre of 0.35 % | Heat-Treated | ASTM A738 | Plate |
Cromo | 0.3 % Show Material materials with Cromo of 0.3 % | Heat-Treated | ASTM A738 | Plate |
Fósforo | 0.025 % Show Material materials with Fósforo of 0.025 % | Heat-Treated | ASTM A738 | Plate |
Manganeso | 0.9 - 1.5 % Show Material materials with Manganeso of 0.9 - 1.5 % | Heat-Treated | ASTM A738 | Plate |
Molibdeno | 0.2 % Show Material materials with Molibdeno of 0.2 % | Heat-Treated | ASTM A738 | Plate |
Niobio | 0.04 % Show Material materials with Niobio of 0.04 % | Heat-Treated | ASTM A738 | Plate |
Níquel | 0.6 % Show Material materials with Níquel of 0.6 % | Heat-Treated | ASTM A738 | Plate |
Silicona | 0.15 - 0.55 % Show Material materials with Silicona of 0.15 - 0.55 % | Heat-Treated | ASTM A738 | Plate |
Vanadio | 0.07 % Show Material materials with Vanadio of 0.07 % | Heat-Treated | ASTM A738 | Plate |
Technological properties
Property | ||
---|---|---|