General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.8 g/cm³ Show Material materials with Densidad of 7.8 g/cm³ | Typical for Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Steel |
Elongación A50 | 23.0 °C | 14 % Show Material materials with Elongación A50 of 14 % | |
Energía de impacto Charpy | 23.0 °C | 41 J Show Material materials with Energía de impacto Charpy of 41 J | |
Estricción | 23.0 °C | 40 % Show Material materials with Estricción of 40 % | |
Módulo elástico | 23.0 °C | 190 - 210 GPa Show Material materials with Módulo elástico of 190 - 210 GPa | Typical for Steel |
Resistencia a la tracción | 23.0 °C | 965 MPa Show Material materials with Resistencia a la tracción of 965 MPa | |
Yield strength Rp0.02 | 23.0 °C | 860 MPa Show Material materials with Yield strength Rp0.02 of 860 MPa |
Chemical properties
Property | Value |
---|---|
Azufre | 0.02 % Show Material materials with Azufre of 0.02 % |
Carbono | 0.45 % Show Material materials with Carbono of 0.45 % |
Cromo | 0.7 - 1.25 % Show Material materials with Cromo of 0.7 - 1.25 % |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % |
Manganeso | 1 % Show Material materials with Manganeso of 1 % |
Molibdeno | 0.2 % Show Material materials with Molibdeno of 0.2 % |
Níquel | 1.65 - 3.5 % Show Material materials with Níquel of 1.65 - 3.5 % |
Silicona | 0.15 - 0.35 % Show Material materials with Silicona of 0.15 - 0.35 % |
Vanadio | 0.07 - 0.12 % Show Material materials with Vanadio of 0.07 - 0.12 % |