General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.8 g/cm³ Show Material materials with Densidad of 7.8 g/cm³ | Typical for Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Steel |
Dureza Brinell | 23.0 °C | 174 - 217 [-] Show Material materials with Dureza Brinell of 174 - 217 [-] | |
Elongación A50 | 23.0 °C | 22 - 25 % Show Material materials with Elongación A50 of 22 - 25 % | |
Estricción | 23.0 °C | 35 - 40 % Show Material materials with Estricción of 35 - 40 % | |
Límite elástico | 23.0 °C | 295 - 305 MPa Show Material materials with Límite elástico of 295 - 305 MPa | |
Módulo elástico | 23.0 °C | 190 - 210 GPa Show Material materials with Módulo elástico of 190 - 210 GPa | Typical for Steel |
Resistencia a la tracción | 23.0 °C | 570 - 585 MPa Show Material materials with Resistencia a la tracción of 570 - 585 MPa |