General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.8 g/cm³ Show Material materials with Densidad of 7.8 g/cm³ | Typical for Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Steel |
Dureza Brinell | 23.0 °C | 174 - 235 [-] Show Material materials with Dureza Brinell of 174 - 235 [-] | |
Elongación A50 | 23.0 °C | 19 - 20 % Show Material materials with Elongación A50 of 19 - 20 % | |
Estricción | 23.0 °C | 36 - 39 % Show Material materials with Estricción of 36 - 39 % | |
Límite elástico | 23.0 °C | 330 - 380 MPa Show Material materials with Límite elástico of 330 - 380 MPa | |
Módulo elástico | 23.0 °C | 190 - 210 GPa Show Material materials with Módulo elástico of 190 - 210 GPa | Typical for Steel |
Resistencia a la tracción | 23.0 °C | 565 - 620 MPa Show Material materials with Resistencia a la tracción of 565 - 620 MPa |