General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.6 - 7.7 g/cm³ Show Material materials with Densidad of 7.6 - 7.7 g/cm³ | Typical for Martensitic Stainless Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Martensitic Stainless Steel |
Dureza Brinell | 23.0 °C | 311 [-] Show Material materials with Dureza Brinell of 311 [-] | |
Dureza Rockwell C | 23.0 °C | 32 [-] Show Material materials with Dureza Rockwell C of 32 [-] | |
Elongación A50 | 23.0 °C | 9 - 13 % Show Material materials with Elongación A50 of 9 - 13 % | |
Energía de impacto Charpy | 23.0 °C | 20 - 27 J Show Material materials with Energía de impacto Charpy of 20 - 27 J | |
Estricción | 23.0 °C | 28 - 45 % Show Material materials with Estricción of 28 - 45 % | |
Límite elástico | 23.0 °C | 860 MPa Show Material materials with Límite elástico of 860 MPa | |
Módulo de cizallamiento | 23.0 °C | 77 GPa Show Material materials with Módulo de cizallamiento of 77 GPa | Typical for Martensitic Stainless Steel |
Módulo elástico | 23.0 °C | 220 GPa Show Material materials with Módulo elástico of 220 GPa | Typical for Martensitic Stainless Steel |
Resistencia a la tracción | 23.0 °C | 1000 MPa Show Material materials with Resistencia a la tracción of 1000 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 460 J/(kg·K) Show Material materials with Calor específico of 460 J/(kg·K) | Typical for Martensitic Stainless Steel |
Coeficiente de dilatación térmica | 23.0 °C | 1E-5 - 1.5E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1E-5 - 1.5E-5 1/K | Typical for Martensitic Stainless Steel |
Conductividad térmica | 23.0 °C | 14 - 31 W/(m·K) Show Material materials with Conductividad térmica of 14 - 31 W/(m·K) | Typical for Martensitic Stainless Steel |
Temperatura de fusión | 1370 - 1530 °C Show Material materials with Temperatura de fusión of 1370 - 1530 °C | Typical for Martensitic Stainless Steel |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Resistividad eléctrica | 23.0 °C | 6E-7 Ω·m Show Material materials with Resistividad eléctrica of 6E-7 Ω·m | Typical for Martensitic Stainless Steel |
Chemical properties
Property | Value |
---|---|
Azufre | 0.03 % Show Material materials with Azufre of 0.03 % |
Carbono | 0.07 % Show Material materials with Carbono of 0.07 % |
Cobre | 2.5 - 4.5 % Show Material materials with Cobre of 2.5 - 4.5 % |
Cromo | 14 - 15.5 % Show Material materials with Cromo of 14 - 15.5 % |
Fósforo | 0.04 % Show Material materials with Fósforo of 0.04 % |
Manganeso | 1 % Show Material materials with Manganeso of 1 % |
Níquel | 3.5 - 5.5 % Show Material materials with Níquel of 3.5 - 5.5 % |
Silicona | 1 % Show Material materials with Silicona of 1 % |