General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 7.85 g/cm³ Show Material materials with Densidad of 7.85 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Steel |
Dureza Brinell | 20.0 °C | 166 - 217 [-] Show Material materials with Dureza Brinell of 166 - 217 [-] | |
Módulo de cizallamiento | 20.0 °C | 81 GPa Show Material materials with Módulo de cizallamiento of 81 GPa | |
Módulo elástico | 20.0 °C | 210 GPa Show Material materials with Módulo elástico of 210 GPa |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Calor específico | 20.0 °C | 460 J/(kg·K) Show Material materials with Calor específico of 460 J/(kg·K) |
Coeficiente de dilatación térmica | 100.0 °C | 1.2E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.2E-5 1/K |
Conductividad térmica | 20.0 °C | 44 W/(m·K) Show Material materials with Conductividad térmica of 44 W/(m·K) |
Chemical properties
Property | Value |
---|---|
Azufre | 0.035 % Show Material materials with Azufre of 0.035 % |
Carbono | 0.14 - 0.2 % Show Material materials with Carbono of 0.14 - 0.2 % |
Cromo | 0.6 - 0.9 % Show Material materials with Cromo of 0.6 - 0.9 % |
Fósforo | 0.03 - 0.04 % Show Material materials with Fósforo of 0.03 - 0.04 % |
Manganeso | 0.4 - 0.7 % Show Material materials with Manganeso of 0.4 - 0.7 % |
Níquel | 3 - 3.5 % Show Material materials with Níquel of 3 - 3.5 % |
Silicona | 0.4 % Show Material materials with Silicona of 0.4 % |