General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.8 - 7.9 g/cm³ Show Material materials with Densidad of 7.8 - 7.9 g/cm³ | Typical for Manganese Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.29 [-] Show Material materials with Coeficiente de Poisson of 0.29 [-] | Typical for Manganese Steel |
Elongación | 20.0 °C | 9 - 12 % Show Material materials with Elongación of 9 - 12 % | |
Límite elástico Rp 0,2 | 20.0 °C | 490 - 710 MPa Show Material materials with Límite elástico Rp 0,2 of 490 - 710 MPa | |
Módulo elástico | 23.0 °C | 200 - 215 GPa Show Material materials with Módulo elástico of 200 - 215 GPa | Typical for Manganese Steel |
Resistencia a la tracción | 20.0 °C | 700 - 1000 MPa Show Material materials with Resistencia a la tracción of 700 - 1000 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 510 - 553 J/(kg·K) Show Material materials with Calor específico of 510 - 553 J/(kg·K) | Typical for Manganese Steel |
Coeficiente de dilatación térmica | 23.0 °C | 1.33E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.33E-5 1/K | Typical for Manganese Steel |
Conductividad térmica | 23.0 °C | 14 - 16 W/(m·K) Show Material materials with Conductividad térmica of 14 - 16 W/(m·K) | Typical for Manganese Steel |
Temperatura de fusión | 1382 - 1529 °C Show Material materials with Temperatura de fusión of 1382 - 1529 °C | Typical for Manganese Steel |
Chemical properties
Property | Value |
---|---|
Azufre | 0.24 - 0.33 % Show Material materials with Azufre of 0.24 - 0.33 % |
Carbono | 0.4 - 0.48 % Show Material materials with Carbono of 0.4 - 0.48 % |
Fósforo | 0.06 % Show Material materials with Fósforo of 0.06 % |
Manganeso | 1.3 - 1.7 % Show Material materials with Manganeso of 1.3 - 1.7 % |
Plomo | 0.15 - 0.35 % Show Material materials with Plomo of 0.15 - 0.35 % |
Silicona | 0.4 % Show Material materials with Silicona of 0.4 % |