General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 20.0 °C | 7.8 - 7.9 g/cm³ Show Material materials with Densidad of 7.8 - 7.9 g/cm³ | Typical for Manganese Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 20.0 °C | 0.29 [-] Show Material materials with Coeficiente de Poisson of 0.29 [-] | Typical for Manganese Steel |
Elongación A80 transversal | 20.0 °C | 26 % Show Material materials with Elongación A80 transversal of 26 % | |
Límite elástico transversal Rp 0,2 | 20.0 °C | 300 - 360 MPa Show Material materials with Límite elástico transversal Rp 0,2 of 300 - 360 MPa | |
Módulo elástico | 20.0 °C | 200 - 215 GPa Show Material materials with Módulo elástico of 200 - 215 GPa | Typical for Manganese Steel |
Resistencia a la tracción transversal | 20.0 °C | 400 - 480 MPa Show Material materials with Resistencia a la tracción transversal of 400 - 480 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 20.0 °C | 510 - 553 J/(kg·K) Show Material materials with Calor específico of 510 - 553 J/(kg·K) | Typical for Manganese Steel |
Coeficiente de dilatación térmica | 20.0 °C | 1.33E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.33E-5 1/K | Typical for Manganese Steel |
Conductividad térmica | 20.0 °C | 14 - 16 W/(m·K) Show Material materials with Conductividad térmica of 14 - 16 W/(m·K) | Typical for Manganese Steel |
Temperatura de fusión | 1382 - 1529 °C Show Material materials with Temperatura de fusión of 1382 - 1529 °C | Typical for Manganese Steel |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.02 % Show Material materials with Aluminio of 0.02 % |
Azufre | 0.025 % Show Material materials with Azufre of 0.025 % |
Carbono | 0.11 % Show Material materials with Carbono of 0.11 % |
Fósforo | 0.12 % Show Material materials with Fósforo of 0.12 % |
Manganeso | 0.7 - 0.8 % Show Material materials with Manganeso of 0.7 - 0.8 % |
Niobio | 0.09 % Show Material materials with Niobio of 0.09 % |
Silicona | 0.5 % Show Material materials with Silicona of 0.5 % |
Titanio | 0.12 % Show Material materials with Titanio of 0.12 % |