General
Property | Value | Comment |
---|---|---|
Densidad | 4.506 g/cm³ Show Material materials with Densidad of 4.506 g/cm³ | Typical for Pure Titanium |
Mecánica
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Coeficiente de Poisson | 0.361 [-] Show Material materials with Coeficiente de Poisson of 0.361 [-] | Typical for Pure Titanium | |||
Elongación | 23.0 % Show Material materials with Elongación of 23.0 % | Hot-Extruded | JIS H4630 | Tube, Pipe | |
Módulo de cizallamiento | 46.0 GPa Show Material materials with Módulo de cizallamiento of 46.0 GPa | Typical for Pure Titanium | |||
Módulo elástico | 120.0 GPa Show Material materials with Módulo elástico of 120.0 GPa | Typical for Pure Titanium | |||
Resistencia a la tracción | 343.0 MPa Show Material materials with Resistencia a la tracción of 343.0 MPa | Hot-Extruded | JIS H4630 | Tube, Pipe |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Calor específico | 513.0 - 599.0 J/(kg·K) Show Material materials with Calor específico of 513.0 - 599.0 J/(kg·K) | Typical for Pure Titanium |
Coeficiente de dilatación térmica | 8.400000000000001e-06 - 8.599999999999999e-06 1/K Show Material materials with Coeficiente de dilatación térmica of 8.400000000000001e-06 - 8.599999999999999e-06 1/K | Typical for Pure Titanium |
Conductividad térmica | 15.0 - 22.0 W/(m·K) Show Material materials with Conductividad térmica of 15.0 - 22.0 W/(m·K) | Typical for Pure Titanium |
Temperatura de fusión | 1670.0 °C Show Material materials with Temperatura de fusión of 1670.0 °C | Typical for Pure Titanium |
Technological properties
Property | ||
---|---|---|
Processing history | hot extruded |