General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.6 - 7.8 g/cm³ Show Material materials with Densidad of 7.6 - 7.8 g/cm³ | Typical for Ferritic Stainless Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Ferritic Stainless Steel |
Dureza Brinell | 23.0 °C | 241 [-] Show Material materials with Dureza Brinell of 241 [-] | |
Dureza Rockwell B | 23.0 °C | 100 [-] Show Material materials with Dureza Rockwell B of 100 [-] | |
Elongación A50 | 23.0 °C | 20 % Show Material materials with Elongación A50 of 20 % | |
Límite elástico | 23.0 °C | 275 MPa Show Material materials with Límite elástico of 275 MPa | |
Módulo de cizallamiento | 23.0 °C | 77 GPa Show Material materials with Módulo de cizallamiento of 77 GPa | Typical for Ferritic Stainless Steel |
Módulo elástico | 23.0 °C | 220 GPa Show Material materials with Módulo elástico of 220 GPa | Typical for Ferritic Stainless Steel |
Resistencia a la tracción | 23.0 °C | 450 MPa Show Material materials with Resistencia a la tracción of 450 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 420 - 586 J/(kg·K) Show Material materials with Calor específico of 420 - 586 J/(kg·K) | Typical for Ferritic Stainless Steel |
Coeficiente de dilatación térmica | 23.0 °C | 9.3E-6 - 1.2E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 9.3E-6 - 1.2E-5 1/K | Typical for Ferritic Stainless Steel |
Conductividad térmica | 23.0 °C | 11 - 22 W/(m·K) Show Material materials with Conductividad térmica of 11 - 22 W/(m·K) | Typical for Ferritic Stainless Steel |
Temperatura de fusión | 1425 - 1530 °C Show Material materials with Temperatura de fusión of 1425 - 1530 °C | Typical for Ferritic Stainless Steel |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Resistividad eléctrica | 23.0 °C | 6E-7 - 7.5E-7 Ω·m Show Material materials with Resistividad eléctrica of 6E-7 - 7.5E-7 Ω·m | Typical for Ferritic Stainless Steel |
Chemical properties
Property | Value |
---|---|
Azufre | 0.02 % Show Material materials with Azufre of 0.02 % |
Carbono | 0.01 % Show Material materials with Carbono of 0.01 % |
Cobre | 0.2 % Show Material materials with Cobre of 0.2 % |
Cromo | 25 - 27.5 % Show Material materials with Cromo of 25 - 27.5 % |
Fósforo | 0.02 % Show Material materials with Fósforo of 0.02 % |
Manganeso | 0.4 % Show Material materials with Manganeso of 0.4 % |
Molibdeno | 0.75 - 1.5 % Show Material materials with Molibdeno of 0.75 - 1.5 % |
Niobio | 0.05 - 0.2 % Show Material materials with Niobio of 0.05 - 0.2 % |
Nitrógeno | 0.02 % Show Material materials with Nitrógeno of 0.02 % |
Níquel | 0.5 % Show Material materials with Níquel of 0.5 % |
Silicona | 0.4 % Show Material materials with Silicona of 0.4 % |