General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.8 g/cm³ Show Material materials with Densidad of 7.8 g/cm³ | Typical for Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Steel |
Elongación A80 transversal | 20.0 °C | 34 - 41 % Show Material materials with Elongación A80 transversal of 34 - 41 % | |
Límite elástico transversal | 20.0 °C | 120 - 170 MPa Show Material materials with Límite elástico transversal of 120 - 170 MPa | |
Módulo elástico | 23.0 °C | 190 - 210 GPa Show Material materials with Módulo elástico of 190 - 210 GPa | Typical for Steel |
Resistencia a la tracción transversal | 20.0 °C | 260 - 350 MPa Show Material materials with Resistencia a la tracción transversal of 260 - 350 MPa |
Chemical properties
Property | Value |
---|---|
Azufre | 0.045 % Show Material materials with Azufre of 0.045 % |
Carbono | 0.12 % Show Material materials with Carbono of 0.12 % |
Fósforo | 0.1 % Show Material materials with Fósforo of 0.1 % |
Manganeso | 0.6 % Show Material materials with Manganeso of 0.6 % |
Silicona | 0.5 % Show Material materials with Silicona of 0.5 % |
Titanio | 0.3 % Show Material materials with Titanio of 0.3 % |