General
Property | Value | Comment |
---|---|---|
Densidad | 7.8 g/cm³ Show Material materials with Densidad of 7.8 g/cm³ | Typical for Steel |
Mecánica
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Coeficiente de Poisson | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Steel | ||||
Elongación | 20.0 °C | 22.0 % Show Material materials with Elongación of 22.0 % | thermomechanically rolled | EN 10225 | Sheet | |
Límite elástico | 20.0 °C | 325.0 MPa Show Material materials with Límite elástico of 325.0 MPa | thermomechanically rolled | EN 10225 | Sheet | |
20.0 °C | 335.0 MPa Show Material materials with Límite elástico of 335.0 MPa | thermomechanically rolled | EN 10225 | Sheet | ||
20.0 °C | 345.0 MPa Show Material materials with Límite elástico of 345.0 MPa | thermomechanically rolled | EN 10225 | Sheet | ||
20.0 °C | 355.0 MPa Show Material materials with Límite elástico of 355.0 MPa | thermomechanically rolled | EN 10225 | Sheet | ||
Módulo elástico | 190.0 - 210.0 GPa Show Material materials with Módulo elástico of 190.0 - 210.0 GPa | Typical for Steel | ||||
Resistencia a la tracción | 20.0 °C | 470.0 - 630.0 MPa Show Material materials with Resistencia a la tracción of 470.0 - 630.0 MPa | thermomechanically rolled | EN 10225 | Sheet |
Aplicaciones térmicas
Property | Value |
---|
Eléctrico
Property | Value |
---|
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Aluminio | 0.015 - 0.055 % Show Material materials with Aluminio of 0.015 - 0.055 % | thermomechanically rolled | EN 10225 | Sheet |
Antimonio | 0.01 Show Material materials with Antimonio of 0.01 | thermomechanically rolled | EN 10225 | Sheet |
Arsénico | 0.03 Show Material materials with Arsénico of 0.03 | thermomechanically rolled | EN 10225 | Sheet |
Azufre | 0.01 Show Material materials with Azufre of 0.01 | thermomechanically rolled | EN 10225 | Sheet |
Bismuto | 0.01 Show Material materials with Bismuto of 0.01 | thermomechanically rolled | EN 10225 | Sheet |
Boro | 0.001 Show Material materials with Boro of 0.001 | thermomechanically rolled | EN 10225 | Sheet |
Calcio | 0.005 Show Material materials with Calcio of 0.005 | thermomechanically rolled | EN 10225 | Sheet |
Carbono | 0.14 Show Material materials with Carbono of 0.14 | thermomechanically rolled | EN 10225 | Sheet |
Cobre | 0.3 Show Material materials with Cobre of 0.3 | thermomechanically rolled | EN 10225 | Sheet |
Cromo | 0.25 Show Material materials with Cromo of 0.25 | thermomechanically rolled | EN 10225 | Sheet |
Estaño | 0.02 Show Material materials with Estaño of 0.02 | thermomechanically rolled | EN 10225 | Sheet |
Fósforo | 0.02 Show Material materials with Fósforo of 0.02 | thermomechanically rolled | EN 10225 | Sheet |
Manganeso | 1.0 - 1.65 % Show Material materials with Manganeso of 1.0 - 1.65 % | thermomechanically rolled | EN 10225 | Sheet |
Molibdeno | 0.08 Show Material materials with Molibdeno of 0.08 | thermomechanically rolled | EN 10225 | Sheet |
Niobio | 0.04 Show Material materials with Niobio of 0.04 | thermomechanically rolled | EN 10225 | Sheet |
Nitrógeno | 0.01 Show Material materials with Nitrógeno of 0.01 | thermomechanically rolled | EN 10225 | Sheet |
Níquel | 0.5 Show Material materials with Níquel of 0.5 | thermomechanically rolled | EN 10225 | Sheet |
Plomo | 0.01 Show Material materials with Plomo of 0.01 | thermomechanically rolled | EN 10225 | Sheet |
Silicona | 0.15 - 0.55 % Show Material materials with Silicona of 0.15 - 0.55 % | thermomechanically rolled | EN 10225 | Sheet |
Titanio | 0.025 Show Material materials with Titanio of 0.025 | thermomechanically rolled | EN 10225 | Sheet |
Vanadio | 0.06 Show Material materials with Vanadio of 0.06 | thermomechanically rolled | EN 10225 | Sheet |
Technological properties
Property | ||
---|---|---|
Supplier Disclaimer | The given information is a rough description and some properties can depend on various factors such as product thickness. Please contact the supplier or refer to the related norm or standard for further information. |