General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.8 g/cm³ Show Material materials with Densidad of 7.8 g/cm³ | Typical for Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Steel |
Elongación | 20.0 °C | 22 % Show Material materials with Elongación of 22 % | |
Límite elástico | 20.0 °C | 345 - 355 MPa Show Material materials with Límite elástico of 345 - 355 MPa | |
Módulo elástico | 23.0 °C | 190 - 210 GPa Show Material materials with Módulo elástico of 190 - 210 GPa | Typical for Steel |
Resistencia a la tracción | 20.0 °C | 460 - 620 MPa Show Material materials with Resistencia a la tracción of 460 - 620 MPa |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.015 - 0.055 % Show Material materials with Aluminio of 0.015 - 0.055 % |
Antimonio | 0.01 % Show Material materials with Antimonio of 0.01 % |
Arsénico | 0.03 % Show Material materials with Arsénico of 0.03 % |
Azufre | 0.015 % Show Material materials with Azufre of 0.015 % |
Bismuto | 0.01 % Show Material materials with Bismuto of 0.01 % |
Boro | 1E-3 % Show Material materials with Boro of 1E-3 % |
Calcio | 5E-3 % Show Material materials with Calcio of 5E-3 % |
Carbono | 0.14 % Show Material materials with Carbono of 0.14 % |
Cobre | 0.3 % Show Material materials with Cobre of 0.3 % |
Cromo | 0.25 % Show Material materials with Cromo of 0.25 % |
Estaño | 0.02 % Show Material materials with Estaño of 0.02 % |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % |
Manganeso | 1.65 % Show Material materials with Manganeso of 1.65 % |
Molibdeno | 0.08 % Show Material materials with Molibdeno of 0.08 % |
Niobio | 0.04 % Show Material materials with Niobio of 0.04 % |
Nitrógeno | 0.01 % Show Material materials with Nitrógeno of 0.01 % |
Níquel | 0.5 % Show Material materials with Níquel of 0.5 % |
Plomo | 0.01 % Show Material materials with Plomo of 0.01 % |
Silicona | 0.55 % Show Material materials with Silicona of 0.55 % |
Titanio | 0.03 % Show Material materials with Titanio of 0.03 % |
Vanadio | 0.06 % Show Material materials with Vanadio of 0.06 % |