General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.8 - 7.9 g/cm³ Show Material materials with Densidad of 7.8 - 7.9 g/cm³ | Typical for Medium Carbon Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.29 [-] Show Material materials with Coeficiente de Poisson of 0.29 [-] | Typical for Medium Carbon Steel |
Módulo de cizallamiento | 23.0 °C | 75 - 80 GPa Show Material materials with Módulo de cizallamiento of 75 - 80 GPa | Typical for Carbon Steel |
Módulo elástico | 23.0 °C | 200 - 215 GPa Show Material materials with Módulo elástico of 200 - 215 GPa | Typical for Medium Carbon Steel |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 470 - 520 J/(kg·K) Show Material materials with Calor específico of 470 - 520 J/(kg·K) | Typical for Medium Carbon Steel |
Coeficiente de dilatación térmica | 23.0 °C | 1.32E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.32E-5 1/K | Typical for Medium Carbon Steel |
Conductividad térmica | 23.0 °C | 21 - 52 W/(m·K) Show Material materials with Conductividad térmica of 21 - 52 W/(m·K) | Typical for Medium Carbon Steel |
Temperatura de fusión | 1380 - 1514 °C Show Material materials with Temperatura de fusión of 1380 - 1514 °C | Typical for Medium Carbon Steel | |
Temperatura máx. de funcionamiento | 500 °C Show Material materials with Temperatura máx. de funcionamiento of 500 °C | Typical for Carbon Steel |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Resistividad eléctrica | 23.0 °C | 1.43E-7 - 1.74E-7 Ω·m Show Material materials with Resistividad eléctrica of 1.43E-7 - 1.74E-7 Ω·m | Typical for Carbon Steel |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.06 % Show Material materials with Aluminio of 0.06 % |
Antimonio | 0.01 % Show Material materials with Antimonio of 0.01 % |
Arsénico | 0.03 % Show Material materials with Arsénico of 0.03 % |
Azufre | 7E-3 % Show Material materials with Azufre of 7E-3 % |
Bismuto | 0.01 % Show Material materials with Bismuto of 0.01 % |
Boro | 1E-3 % Show Material materials with Boro of 1E-3 % |
Calcio | 5E-3 % Show Material materials with Calcio of 5E-3 % |
Carbono | 0.18 % Show Material materials with Carbono of 0.18 % |
Cobre | 0.35 % Show Material materials with Cobre of 0.35 % |
Cromo | 0.25 % Show Material materials with Cromo of 0.25 % |
Estaño | 0.02 % Show Material materials with Estaño of 0.02 % |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % |
Manganeso | 1.6 % Show Material materials with Manganeso of 1.6 % |
Molibdeno | 0.08 % Show Material materials with Molibdeno of 0.08 % |
Niobio | 0.05 % Show Material materials with Niobio of 0.05 % |
Nitrógeno | 0.01 % Show Material materials with Nitrógeno of 0.01 % |
Níquel | 0.3 % Show Material materials with Níquel of 0.3 % |
Plomo | 0.01 % Show Material materials with Plomo of 0.01 % |
Silicona | 0.15 - 0.55 % Show Material materials with Silicona of 0.15 - 0.55 % |
Titanio | 0.02 % Show Material materials with Titanio of 0.02 % |
Vanadio | 0.1 % Show Material materials with Vanadio of 0.1 % |