General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.7 - 8.7 g/cm³ Show Material materials with Densidad of 7.7 - 8.7 g/cm³ | Typical for Leaded Phosphor Bronze |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Leaded Phosphor Bronze |
Dureza Rockwell B | 23.0 °C | 74 - 96 [-] Show Material materials with Dureza Rockwell B of 74 - 96 [-] | |
Hardness, Rockwell Superficial 30-T | 23.0 °C | 59 - 77 [-] Show Material materials with Hardness, Rockwell Superficial 30-T of 59 - 77 [-] | |
Módulo elástico | 23.0 °C | 110 - 130 GPa Show Material materials with Módulo elástico of 110 - 130 GPa | Typical for Leaded Phosphor Bronze |
Resistencia a la tracción | 23.0 °C | 525 - 625 MPa Show Material materials with Resistencia a la tracción of 525 - 625 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 380 J/(kg·K) Show Material materials with Calor específico of 380 J/(kg·K) | Typical for Leaded Phosphor Bronze |
Coeficiente de dilatación térmica | 23.0 °C | 1.5E-5 - 1.9E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.5E-5 - 1.9E-5 1/K | Typical for Leaded Phosphor Bronze |
Chemical properties
Property | Value |
---|---|
Estaño | 9 - 11 % Show Material materials with Estaño of 9 - 11 % |
Fósforo | 0.03 - 0.35 % Show Material materials with Fósforo of 0.03 - 0.35 % |
Hierro | 0.1 % Show Material materials with Hierro of 0.1 % |
Plomo | 0.05 % Show Material materials with Plomo of 0.05 % |
Zinc | 0.2 % Show Material materials with Zinc of 0.2 % |