To be a model rolling mill in the world, with its environment-friendliness as well as the highest level of working environment
HARADA started manufacturing and sales of phosphor bronze materials soon after its establishment in 1952, and became only one manufacturer in the world specialized to phosphor bronze in 1970, based on its business consolidation in view of promising future of phosphor bronze as a nonferrous metal.
CDA: C50500, C51100, C51000, C51900, C52100, C52400
Product Features
High Quality Phosphor Bronze (HQ) C51900, C52100, C52400
-High Quality Phosphor Bronze is upper grade of normal Phosphor Bronze.
-Small Grain Size 3μm or below.
-Superior mechanical properties.
-Excellent high Tensile Strength and Yield strength (C5240HQ-XSH TS 1,063N/㎟ YS1,025N/㎟).
-Excellent bendability.
-Main application are micro connectors for worldwide global electronics parts & other communication devices maker.
High precision Extra Thin material
-Minimum thickness is 0.05mm(0.00197”)
-Highest level of thickness tolerance control.
-Highest level of consistency for mechanical properties.
Hot Dip Tin plating
- Only manufacturer of Hot Dip Tin Plating in Japan.
- Available thick plating thickness up to 8.0 (μm)
- High whisker resistance, preventive measures for short circuit accidents
- High adhesion, intermediate alloy layer is formed between phosphor bronze and tin plating during plating to achieve high adhesion
To meet the customers’ ultimate expectations, HARADA has implemented its investment in plant facilities as well as its production systems based on a long –term plan, such as the consolidation of the whole production process (melting, casting, rolling, annealing, surface treatment, leveling and other ancillary processes) into Sendai factory as an integrated production line.
HOT-DIP-tinning, a metallurgically completely different from electroplating, has very low occurrence of whiskers, provides extremely strong adhesion to the base metal, achieves superb bend workability, and has high reliability particularly as material for small-sized high-density components, for example.
HARADA has enabled automatic control of optional thickness by applying the cutting-edge technology of Hot Air Level System to this tested HOT-DIP-tinning manufacturing and has achieved higher productivity of uniformly bright surface finished products.
Sede
Saitama, Japan
Ingresos
11-100M USD
Número de empleados
101-200
Año de creación
1952
Tipo
Fabricante y distribuidor
Certificados de calidad
ISO 90001/ ISO 14001
Además: Wrought Copper Bronze
Accesorios eléctricos
Actuadores
Aeroespacial
Aislamiento
Alambres y cables
Armarios eléctricos
Auto Electronics
Automotriz
Barras
Baterías
Battery Contacts
Bearings General
Bicycle Frames
Bicycles & Parts
Bolsa de aire
Bonding
Capacitors In General
Car Controls
Car Informatics
Ciencias
Cierres
Clamps & Staples
Climatización
Cojinetes
Componentes electrónicos
Componentes electrónicos de un coche
Componentes para equipos eléctricos
Comunicaciones
Condensadores
Conduits For Electrical Purposes
Conexiones
Construcción
Contactos eléctricos
Copper & Copper Alloys
Copper Products
Diodos
Disipadores de calor
Dispositivos de conexión
Dispositivos semiconductores
E-Motor
Electric & Electromechanical
Electrical & Electronic Testing
Electrical Equipment In Special Conditions
Electrical Installations For Outdoor Use
Electricity Supply Systems
Electro Mechanical Components
Electronic Devices
Electrónica
Elementos de sujeción
Emi Shielding
Enchufes
Energía
Energía solar
Engranajes
Equipo de telecomunicaciones
Equipos de protección
Estructura de carrocería
Eyewear Parts
Fabricación
Fasteners General
Ferrocarriles
Fijadores para el sector aeroespacial
Fotovoltaicos
Fusibles y Ocp
Horología
Iluminación de automóviles
Industria textil
Ingeniería eléctrica
Instalaciones en edificios
Instalaciones sanitarias
Interruptores
Joyería
Keys & Splines
Leadframes
Leds
Lámparas
Lámparas y equipos relacionados
Materiales aeroespaciales
Mecánica de precisión
Metalurgia
Metrología
Microelectrónica
Microprocessors
Monturas para gafas
Motorcycle Body Components
Motorcycles
Motores de combustión
Motores eléctricos
Muelles
Non-Ferrous Alloys
Non-Ferrous Metals
Non-Ferrous Metals In General
Non-Ferrous Products
Optoelectrónica
Other Electrical Accessories
Other Fasteners
Other Semiconductor Devices
Physics Chemistry
Piezas generales para vehículos
Plain Bearings
Grade | Shape | ||
---|---|---|---|
HRD125 Harada | Plate, Strip | HRD125, JIS C5050, UNS C50500 | JIS H3110 |
HRD200 Harada | Plate, Strip | HRD200 | JIS H3110 |
JIS C5102 Harada | Plate, Strip | JIS C5102, CDA C51000, UNS C51000, BS PB102, EN CW451K, ASTM C51000 | JIS H3110, ASTM B103, EN 1652, EN 1653 |
JIS C5111 Harada | Plate, Strip | JIS C5111, CDA C51100, UNS C51100, BS PB101, DIN CuSn4, EN CW450K, GB QSn4-0.3, ASTM C51100 | JIS H3110, ASTM B103, DIN 17662-1, DIN 17670-1, EN 1652, EN 1653, GB 2066 |
JIS C5191 Harada | Plate, Strip | JIS C5191, UNS C51900, BS PB103, DIN CuSn6, EN CW452K, GB QSn6.5-0.1, GB QSn6.5-0.4, GB QSn7-0.2 | JIS H3110, DIN 17662-1, DIN 17670-1, EN 1652, EN 1653, GB 2066 |
JIS C5191HQ Harada | Plate, Strip | JIS C5191HQ, CDA C51900, BS PB103, DIN CuSn6, EN CW452K, GB QSn6.5-0.1, GB QSn6.5-0.4, GB QSn7-0.2, ASTM C51900 | JIS H3110, DIN 17662-1, DIN 17670-1, EN 1652, EN 1653, GB 2066 |
JIS C5210 Harada | Plate, Strip | JIS C5210, CDA C52100, UNS C52100, BS PB104, DIN CuSn8, EN CW453K, GB QSn8-0.3, ASTM C52100 | JIS H3130, ASTM B103, DIN 17662-1, DIN 17670-1, EN 1652, EN 1653, GB 2066 |
JIS C5210HQ Harada | Plate, Strip | JIS C5210HQ, CDA C52100, UNS C52100, BS PB104, DIN CuSn8, EN CW453K, GB QSn8-0.3, ASTM C52100 | JIS H3110, ASTM B103, DIN 17662-1, DIN 17670-1, EN 1652, EN 1653, GB 2066 |
JIS C5212 Harada | Plate, Strip | JIS C5212, CDA C52100, UNS C52100, BS PB104, DIN CuSn8, EN CW453K, GB QSn8-0.3 | JIS H3110, ASTM B103, DIN 17662-1, DIN 17670-1, EN 1652, EN 1653, GB 2066 |
JIS C5240 Harada | Plate, Strip | JIS C5240, CDA C52400, UNS C52400, DIN CuSn10, ASTM C52400 | JIS H3130, ASTM B103, DIN 17662-1, DIN 17670-1 |