EN 1652 Grade CuZn39Pb0.5 H165

View suppliers (3)
Want to keep this datasheet? Save it now in your required format

Description

Material CuZn39Pb0,5, mat. No. CW610N, is an unhardenable wrought alloy. to the comparable make CuZn39Pb0,5, mat. No. 2.0372 acc. to DIN 17660 : 1983-12 applies: High hardness and strength parameter are achievable by cold forming only. Thermal and electrical conductivity are lower than for the unleaded brass grade of the same Zn-content. Machinability is improved by Pb-addition. Corrosion resistance to water, several saline solutions and organic liquids is also lower than for unleaded alloys of the same zinc-content. Processing properties: warm forming: very good cold forming: moderately machinability: good hard soldering: moderately soft soldering: very good TIG-welding: moderately burnishing: very good Application: For plug pins, fitting parts, rivets, condenser plates, floor plate screeding and drawing instruments.

Related Standards

Equivalent Materials

Los datos sobre este material han sido proporcionados por WIAM.

A menos que se indique lo contrario, todas las medidas corresponden a condiciones de temperatura ambiente. A menos que se indique lo contrario, se utilizan las unidades del SI.
Las normas armonizadas son similares a uno o varios estándares del proveedor. Es posible que algunas normas armonizadas se ajusten al estándar original, mientras que otras pueden quedar fuera de su alcance.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Propiedades

General

PropertyTemperatureValue

Densidad

20.0 °C

8.4 g/cm³

Show Material materials with Densidad of 8.4 g/cm³

Mecánica

PropertyTemperatureValue

Dureza Vickers

20.0 °C

165 [-]

Show Material materials with Dureza Vickers of 165 [-]

Módulo de cizallamiento

20.0 °C

37 GPa

Show Material materials with Módulo de cizallamiento of 37 GPa

Módulo elástico

20.0 °C

102 GPa

Show Material materials with Módulo elástico of 102 GPa

Aplicaciones térmicas

PropertyTemperatureValueComment

Calor específico

23.0 °C

371 - 418 J/(kg·K)

Show Material materials with Calor específico of 371 - 418 J/(kg·K)

Typical for Wrought Copper Brass

Coeficiente de dilatación térmica

200.0 °C

2.04E-5 1/K

Show Material materials with Coeficiente de dilatación térmica of 2.04E-5 1/K

Conductividad térmica

20.0 °C

109 W/(m·K)

Show Material materials with Conductividad térmica of 109 W/(m·K)

Temperatura de fusión

875 - 1075 °C

Show Material materials with Temperatura de fusión of 875 - 1075 °C

Typical for Wrought Copper Brass

Eléctrico

PropertyTemperatureValue

Conductividad eléctrica

20.0 °C

1.39E+7 S/m

Show Material materials with Conductividad eléctrica of 1.39E+7 S/m

Resistividad eléctrica

20.0 °C

7.2E-8 Ω·m

Show Material materials with Resistividad eléctrica of 7.2E-8 Ω·m

Chemical properties

PropertyValue

Aluminio

0.05 %

Show Material materials with Aluminio of 0.05 %

Cobre

59 - 60.5 %

Show Material materials with Cobre of 59 - 60.5 %

Estaño

0.2 %

Show Material materials with Estaño of 0.2 %

Hierro

0.2 %

Show Material materials with Hierro of 0.2 %

Níquel

0.3 %

Show Material materials with Níquel of 0.3 %

Plomo

0.2 - 0.8 %

Show Material materials with Plomo of 0.2 - 0.8 %