General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 7.6 g/cm³ Show Material materials with Densidad of 7.6 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Leaded Phosphor Bronze |
Dureza Vickers | 20.0 °C | 160 [-] Show Material materials with Dureza Vickers of 160 [-] | |
Elongación | 20.0 °C | 14 % Show Material materials with Elongación of 14 % | |
Límite elástico Rp 0,2 | 20.0 °C | 230 MPa Show Material materials with Límite elástico Rp 0,2 of 230 MPa | |
Módulo de cizallamiento | 20.0 °C | 45 GPa Show Material materials with Módulo de cizallamiento of 45 GPa | |
Módulo elástico | -253.0 °C | 128 GPa Show Material materials with Módulo elástico of 128 GPa | |
-195.0 °C | 123 GPa Show Material materials with Módulo elástico of 123 GPa | ||
-100.0 °C | 122 GPa Show Material materials with Módulo elástico of 122 GPa | ||
20.0 °C | 120 GPa Show Material materials with Módulo elástico of 120 GPa | ||
50.0 °C | 120 GPa Show Material materials with Módulo elástico of 120 GPa | ||
100.0 °C | 116 GPa Show Material materials with Módulo elástico of 116 GPa | ||
150.0 °C | 115 GPa Show Material materials with Módulo elástico of 115 GPa | ||
200.0 °C | 115 GPa Show Material materials with Módulo elástico of 115 GPa | ||
250.0 °C | 110 GPa Show Material materials with Módulo elástico of 110 GPa | ||
Resistencia a la tracción | 20.0 °C | 590 MPa Show Material materials with Resistencia a la tracción of 590 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 20.0 °C | 420 J/(kg·K) Show Material materials with Calor específico of 420 J/(kg·K) | |
Coeficiente de dilatación térmica | 23.0 °C | 1.5E-5 - 1.9E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.5E-5 - 1.9E-5 1/K | Typical for Leaded Phosphor Bronze |
Conductividad térmica | 20.0 °C | 50 - 57 W/(m·K) Show Material materials with Conductividad térmica of 50 - 57 W/(m·K) |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 20.0 °C | 4.00E+6 - 7.00E+6 S/m Show Material materials with Conductividad eléctrica of 4.00E+6 - 7.00E+6 S/m |
Specific Electrical conductivity | 10.3 % IACS Show Material materials with Specific Electrical conductivity of 10.3 % IACS |
Chemical properties
Property | Value |
---|---|
Aluminio | 8.5 - 11 % Show Material materials with Aluminio of 8.5 - 11 % |
Estaño | 0.1 % Show Material materials with Estaño of 0.1 % |
Hierro | 3 - 5 % Show Material materials with Hierro of 3 - 5 % |
Manganeso | 1 % Show Material materials with Manganeso of 1 % |
Níquel | 4 - 6 % Show Material materials with Níquel of 4 - 6 % |
Plomo | 0.05 % Show Material materials with Plomo of 0.05 % |
Silicona | 0.2 % Show Material materials with Silicona of 0.2 % |
Zinc | 0.4 % Show Material materials with Zinc of 0.4 % |