General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 8.35 - 8.4 g/cm³ Show Material materials with Densidad of 8.35 - 8.4 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Vickers | 20.0 °C | 85 [-] Show Material materials with Dureza Vickers of 85 [-] |
Elongación | 20.0 °C | 20 - 30 % Show Material materials with Elongación of 20 - 30 % |
Elongation A10 | 20.0 °C | 25 % Show Material materials with Elongation A10 of 25 % |
Elongation A100 | 20.0 °C | 10 % Show Material materials with Elongation A100 of 10 % |
Elongation A11.3 | 20.0 °C | 15 % Show Material materials with Elongation A11.3 of 15 % |
Límite elástico Rp 0,2 | 20.0 °C | 120 - 170 MPa Show Material materials with Límite elástico Rp 0,2 of 120 - 170 MPa |
Límite elástico Rp 1,0 | 50.0 °C | 160 - 175 MPa Show Material materials with Límite elástico Rp 1,0 of 160 - 175 MPa |
100.0 °C | 153 - 172 MPa Show Material materials with Límite elástico Rp 1,0 of 153 - 172 MPa | |
150.0 °C | 148 - 168 MPa Show Material materials with Límite elástico Rp 1,0 of 148 - 168 MPa | |
Módulo de cizallamiento | 20.0 °C | 42 GPa Show Material materials with Módulo de cizallamiento of 42 GPa |
Módulo elástico | 20.0 °C | 112 GPa Show Material materials with Módulo elástico of 112 GPa |
Resistencia a la tracción | 20.0 °C | 340 MPa Show Material materials with Resistencia a la tracción of 340 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 371 - 418 J/(kg·K) Show Material materials with Calor específico of 371 - 418 J/(kg·K) | Typical for Wrought Copper Brass |
Coeficiente de dilatación térmica | 23.0 °C | 1.7E-5 - 2.1E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.7E-5 - 2.1E-5 1/K | Typical for Wrought Copper Brass |
Conductividad térmica | 20.0 °C | 117 W/(m·K) Show Material materials with Conductividad térmica of 117 W/(m·K) | |
Temperatura de fusión | 875 - 1075 °C Show Material materials with Temperatura de fusión of 875 - 1075 °C | Typical for Wrought Copper Brass |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 20.0 °C | 1.51E+7 S/m Show Material materials with Conductividad eléctrica of 1.51E+7 S/m |
Resistividad eléctrica | 20.0 °C | 6.6E-8 Ω·m Show Material materials with Resistividad eléctrica of 6.6E-8 Ω·m |
Chemical properties
Property | Value |
---|---|
Cobre | 59 - 61 % Show Material materials with Cobre of 59 - 61 % |
Estaño | 0.5 - 1 % Show Material materials with Estaño of 0.5 - 1 % |
Hierro | 0.1 % Show Material materials with Hierro of 0.1 % |
Níquel | 0.2 % Show Material materials with Níquel of 0.2 % |
Plomo | 0.2 % Show Material materials with Plomo of 0.2 % |