EN 12163 Grade CuCo2Be M

View suppliers (3)
Want to keep this datasheet? Save it now in your required format

Description

Cuco2Be, mat. No CW104C, is counted among hardenable, low alloyed copper alloys. To the comparable make Cuco2Be, mat. No 2.1285, acc. to DIN 17666 : 1983-12 applies: CuCo2Be achieves compared to CuBe2 at slightly lower hardness and strength values higher electrical and thermal conductivity. The temperature for removal of workhardening approximates 500°C, high corrosion resistance. Processing properties: hot and cold forming: good machinability: moderately hard and soft soldering: good gas shielded welding: good burnishing: good Application: In relay and switch construction for high loadable, live springs and for radiant heaters at semi conductors. Furthermore for resistance and welding electrodes as well as for pistons, plunger and punching tools. For the electrolytically tinned strip the coatings (Sn bright, Sn matt, Sn fuzed, SnPb) are listed by the application (better solderability, better corrosion resistance, reduction of the electrical contact resistance, better appearance) in the DIN EN 14436 : 2004-11 (Table 5)

Related Standards

Equivalent Materials

Los datos sobre este material han sido proporcionados por WIAM.

A menos que se indique lo contrario, todas las medidas corresponden a condiciones de temperatura ambiente. A menos que se indique lo contrario, se utilizan las unidades del SI.
Las normas armonizadas son similares a uno o varios estándares del proveedor. Es posible que algunas normas armonizadas se ajusten al estándar original, mientras que otras pueden quedar fuera de su alcance.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Propiedades

General

PropertyTemperatureValue

Densidad

20.0 °C

8.8 g/cm³

Show Material materials with Densidad of 8.8 g/cm³

Mecánica

PropertyTemperatureValueComment

Dureza Brinell

20.0 °C

60 [-]

Show Material materials with Dureza Brinell of 60 [-]

Dureza Vickers

20.0 °C

65 [-]

Show Material materials with Dureza Vickers of 65 [-]

Límite elástico Rp 0,2

20.0 °C

200 MPa

Show Material materials with Límite elástico Rp 0,2 of 200 MPa

Módulo elástico

23.0 °C

110 - 130 GPa

Show Material materials with Módulo elástico of 110 - 130 GPa

Typical for Wrought Copper High Copper Alloy

Resistencia a la tracción

20.0 °C

300 MPa

Show Material materials with Resistencia a la tracción of 300 MPa

Aplicaciones térmicas

PropertyTemperatureValueComment

Calor específico

23.0 °C

360 - 420 J/(kg·K)

Show Material materials with Calor específico of 360 - 420 J/(kg·K)

Typical for Wrought Copper High Copper Alloy

Coeficiente de dilatación térmica

23.0 °C

1.6E-5 - 1.8E-5 1/K

Show Material materials with Coeficiente de dilatación térmica of 1.6E-5 - 1.8E-5 1/K

Typical for Wrought Copper High Copper Alloy

Temperatura de fusión

855 - 1090 °C

Show Material materials with Temperatura de fusión of 855 - 1090 °C

Typical for Wrought Copper High Copper Alloy

Temperatura máx. de funcionamiento, largo

0 - 350 °C

Show Material materials with Temperatura máx. de funcionamiento, largo of 0 - 350 °C

Chemical properties

PropertyValue

Berilio

0.4 - 0.7 %

Show Material materials with Berilio of 0.4 - 0.7 %

Cobalto

2 - 2.8 %

Show Material materials with Cobalto of 2 - 2.8 %

Hierro

0.2 %

Show Material materials with Hierro of 0.2 %

Níquel

0.3 %

Show Material materials with Níquel of 0.3 %