Wrought Copper High Copper Alloy
ASTM B534 Grade C17500 TB00Wrought Copper High Copper Alloy
ASTM B534 Grade C17500 TF00Wrought Copper High Copper Alloy
ASTM B441 Grade C17500 TH04Wrought Copper High Copper Alloy
ASTM B534 Grade C17500 TD04Aleación níquel-cobre
DIN 17743 Grade NiCu30Fe soft annealed (+A)Wrought Copper High Copper Alloy
Alloy 10 (C17500)TB00 Rod and BarSuministrada por:
Materion Brush GmbHWrought Copper High Copper Alloy
Alloy 10 (C17500) TD04 Rod and BarSuministrada por:
Materion Brush GmbHWrought Copper High Copper Alloy
Alloy 10 (C17500)TF00 Rod and BarSuministrada por:
Materion Brush GmbHWrought Copper High Copper Alloy
Alloy 10 (C17500) TH04 Rod and BarSuministrada por:
Materion Brush GmbHWrought Copper High Copper Alloy
EN 1652 Grade CuCo2Be TH