General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 8.9 g/cm³ Show Material materials with Densidad of 8.9 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Brinell | 20.0 °C | 65 - 90 [-] Show Material materials with Dureza Brinell of 65 - 90 [-] | |
Dureza Vickers | 20.0 °C | 70 - 95 [-] Show Material materials with Dureza Vickers of 70 - 95 [-] | |
Elongación | 20.0 °C | 30 % Show Material materials with Elongación of 30 % | |
Límite elástico Rp 0,2 | 20.0 °C | 60 MPa Show Material materials with Límite elástico Rp 0,2 of 60 MPa | |
Módulo elástico | 23.0 °C | 110 - 130 GPa Show Material materials with Módulo elástico of 110 - 130 GPa | Typical for Wrought Copper High Copper Alloy |
Resistencia a la tracción | 20.0 °C | 200 MPa Show Material materials with Resistencia a la tracción of 200 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 360 - 420 J/(kg·K) Show Material materials with Calor específico of 360 - 420 J/(kg·K) | Typical for Wrought Copper High Copper Alloy |
Coeficiente de dilatación térmica | 23.0 °C | 1.6E-5 - 1.8E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.6E-5 - 1.8E-5 1/K | Typical for Wrought Copper High Copper Alloy |
Temperatura de fusión | 855 - 1090 °C Show Material materials with Temperatura de fusión of 855 - 1090 °C | Typical for Wrought Copper High Copper Alloy |
Chemical properties
Property | Value |
---|---|
Cromo | 0.5 - 1.2 % Show Material materials with Cromo of 0.5 - 1.2 % |
Hierro | 0.08 % Show Material materials with Hierro of 0.08 % |
Silicona | 0.1 % Show Material materials with Silicona of 0.1 % |