General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 8.8 - 8.9 g/cm³ Show Material materials with Densidad of 8.8 - 8.9 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Brinell | 20.0 °C | 50 - 180 [-] Show Material materials with Dureza Brinell of 50 - 180 [-] | |
Dureza Vickers | 20.0 °C | 50 [-] Show Material materials with Dureza Vickers of 50 [-] | |
Límite elástico Rp 0,2 | 20.0 °C | 200 MPa Show Material materials with Límite elástico Rp 0,2 of 200 MPa | |
Módulo elástico | 23.0 °C | 110 - 130 GPa Show Material materials with Módulo elástico of 110 - 130 GPa | Typical for Wrought Copper High Copper Alloy |
Resistencia a la tracción | 20.0 °C | 300 MPa Show Material materials with Resistencia a la tracción of 300 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 20.0 °C | 377 J/(kg·K) Show Material materials with Calor específico of 377 J/(kg·K) | |
Coeficiente de dilatación térmica | 300.0 °C | 1.68E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.68E-5 1/K | |
Temperatura de fusión | 855 - 1090 °C Show Material materials with Temperatura de fusión of 855 - 1090 °C | Typical for Wrought Copper High Copper Alloy |
Chemical properties
Property | Value |
---|---|
Hierro | 0.2 % Show Material materials with Hierro of 0.2 % |
Manganeso | 0.1 % Show Material materials with Manganeso of 0.1 % |
Níquel | 1 - 1.6 % Show Material materials with Níquel of 1 - 1.6 % |
Plomo | 0.02 % Show Material materials with Plomo of 0.02 % |
Silicona | 0.4 - 0.7 % Show Material materials with Silicona of 0.4 - 0.7 % |